Loading…
Properties of boron-rich slag separated from boron-bearing iron concentrate
In the present paper, the fundamental research on the properties of boron-rich slag melting separated from boron-bearing iron concentrate was performed. The melting and fluidity of B 2 O 3 -MgO-SiO 2 -FeO slag system, crystallization of separated boron-rich slag and factors on the extraction efficie...
Saved in:
Published in: | Journal of Central South University 2018-04, Vol.25 (4), p.783-794 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | In the present paper, the fundamental research on the properties of boron-rich slag melting separated from boron-bearing iron concentrate was performed. The melting and fluidity of B
2
O
3
-MgO-SiO
2
-FeO slag system, crystallization of separated boron-rich slag and factors on the extraction efficiency of boron-rich slag were systematically investigated. B
2
O
3
content would heavily affect the melting and fluidity property of boron-rich slag. Generally, FeO could improve the melting and fluidity property of boron-rich slag. Boron-containing crystalline phase mainly precipitated in temperature range from 1200 °C to 1100 °C. Higher smelting temperature and B2O3 reduction ratio were negative for the extraction of boron. The cooling rate of 10–20 °C/min was better for the crystallization of boron-containing crystalline phase. Based on the obtained experimental results, the optimum operating parameters for the development of pyrometallurgical boron and iron separation process and further boron-rich slag cooling process were proposed. |
---|---|