Loading…
Mitigation and control of the overcuring effect in mask projection micro-stereolithography
Mask Projection micro-Stereolithography (MPμSL) is an additive manufacturing technique capable of producing solid parts with micron-scale resolution from a vat of photocurable liquid polymer resin. Although the physical mechanism remains the same, the process differs from traditional laser-galvanome...
Saved in:
Main Authors: | , , |
---|---|
Format: | Conference Proceeding |
Language: | English |
Subjects: | |
Citations: | Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | cdi_FETCH-LOGICAL-c328t-c42a0c69d1d008541b7ad39a19b11981096276a43075974e43176d026327b0213 |
---|---|
cites | |
container_end_page | |
container_issue | 1 |
container_start_page | |
container_title | |
container_volume | 1896 |
creator | O'Neill, Paul F. Kent, Nigel Brabazon, Dermot |
description | Mask Projection micro-Stereolithography (MPμSL) is an additive manufacturing technique capable of producing solid parts with micron-scale resolution from a vat of photocurable liquid polymer resin. Although the physical mechanism remains the same, the process differs from traditional laser-galvanometer based stereolithography (SL) in its use of a dynamic mask UV projector, or digital light processor (DLP), which cures each location within each 3D layer at the same time. One area where MPµSL has garnered considerable attention is in the field of microfluidics and Lab-on-a-Chip, where complex multistep microfabrication techniques adopted from the semiconductor industry are still widely used, and where MPµSL offers the ability to fabricate completely encapsulated fluidic channels in a single step and at low cost [1–3]. However, a significant obstacle exists in the prevention of channel blockage due to overcuring of the polymer resin [4, 5]. Overcuring can be attributed to the so-called ‘back side effect’ [2] which occurs during the build process as light from successive layers penetrates into the resin to a depth greater than the layer thickness. This effect is most prevalent in channels or features oriented horizontally (in a parallel plane to that of the build platform). Currently there are two main approaches in controlling the cure depth; 1. the chemical approach, which involves doping the resin material with a chemical light absorber [6–8]; and 2. by improving the system's hardware and optical elements to improve the homogeneity of the light dosage and control the cure depth [9]. Here we investigate a third approach through modification of the 3D CAD file prior to printing to mitigate for UV light leakage from successive build layers. Although used here in conjunction with the MPμSL technique, this approach can be applied to a range of SL techniques to improve printer resolution and enable production of internal features with higher dimensional accuracy. |
doi_str_mv | 10.1063/1.5008249 |
format | conference_proceeding |
fullrecord | <record><control><sourceid>proquest_scita</sourceid><recordid>TN_cdi_proquest_journals_2116042653</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>2116042653</sourcerecordid><originalsourceid>FETCH-LOGICAL-c328t-c42a0c69d1d008541b7ad39a19b11981096276a43075974e43176d026327b0213</originalsourceid><addsrcrecordid>eNp9kE9LAzEQxYMoWKsHv0HAm7B1Jskmm6MU_0HFi4J4CWk226a2m5pNC_32brXgzdMw8Hsz7z1CLhFGCJLf4KgEqJjQR2SAZYmFkiiPyQBAi4IJ_n5KzrpuAcC0UtWAfDyHHGY2h9hS29bUxTanuKSxoXnuadz65DYptDPqm8a7TENLV7b7pOsUF_2-162CS7Hosk8-LkOex1my6_nunJw0dtn5i8Mckrf7u9fxYzF5eXga304Kx1mVCyeYBSd1jXXvvBQ4Vbbm2qKeIuoKQUumpBUcVKmV8IKjkjUwyZmaAkM-JFe_d3tLXxvfZbOIm9T2Lw1DlCCYLHlPXf9SnQv5J69Zp7CyaWe2MRk0h97Mum7-gxHMvug_Af8GEoxurQ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>conference_proceeding</recordtype><pqid>2116042653</pqid></control><display><type>conference_proceeding</type><title>Mitigation and control of the overcuring effect in mask projection micro-stereolithography</title><source>American Institute of Physics:Jisc Collections:Transitional Journals Agreement 2021-23 (Reading list)</source><creator>O'Neill, Paul F. ; Kent, Nigel ; Brabazon, Dermot</creator><contributor>Ahad, Inam Ul ; Brabazon, Dermot ; Naher, Sumsun</contributor><creatorcontrib>O'Neill, Paul F. ; Kent, Nigel ; Brabazon, Dermot ; Ahad, Inam Ul ; Brabazon, Dermot ; Naher, Sumsun</creatorcontrib><description>Mask Projection micro-Stereolithography (MPμSL) is an additive manufacturing technique capable of producing solid parts with micron-scale resolution from a vat of photocurable liquid polymer resin. Although the physical mechanism remains the same, the process differs from traditional laser-galvanometer based stereolithography (SL) in its use of a dynamic mask UV projector, or digital light processor (DLP), which cures each location within each 3D layer at the same time. One area where MPµSL has garnered considerable attention is in the field of microfluidics and Lab-on-a-Chip, where complex multistep microfabrication techniques adopted from the semiconductor industry are still widely used, and where MPµSL offers the ability to fabricate completely encapsulated fluidic channels in a single step and at low cost [1–3]. However, a significant obstacle exists in the prevention of channel blockage due to overcuring of the polymer resin [4, 5]. Overcuring can be attributed to the so-called ‘back side effect’ [2] which occurs during the build process as light from successive layers penetrates into the resin to a depth greater than the layer thickness. This effect is most prevalent in channels or features oriented horizontally (in a parallel plane to that of the build platform). Currently there are two main approaches in controlling the cure depth; 1. the chemical approach, which involves doping the resin material with a chemical light absorber [6–8]; and 2. by improving the system's hardware and optical elements to improve the homogeneity of the light dosage and control the cure depth [9]. Here we investigate a third approach through modification of the 3D CAD file prior to printing to mitigate for UV light leakage from successive build layers. Although used here in conjunction with the MPμSL technique, this approach can be applied to a range of SL techniques to improve printer resolution and enable production of internal features with higher dimensional accuracy.</description><identifier>ISSN: 0094-243X</identifier><identifier>EISSN: 1551-7616</identifier><identifier>DOI: 10.1063/1.5008249</identifier><identifier>CODEN: APCPCS</identifier><language>eng</language><publisher>Melville: American Institute of Physics</publisher><subject>Channels ; Cures ; Galvanometers ; Lithography ; Microfluidics ; Microprocessors ; Optical components ; Organic chemistry ; Rapid prototyping ; Thickness ; Ultraviolet radiation</subject><ispartof>AIP conference proceedings, 2017, Vol.1896 (1)</ispartof><rights>Author(s)</rights><rights>2017 Author(s). Published by AIP Publishing.</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c328t-c42a0c69d1d008541b7ad39a19b11981096276a43075974e43176d026327b0213</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>309,310,314,780,784,789,790,23928,23929,25138,27922,27923</link.rule.ids></links><search><contributor>Ahad, Inam Ul</contributor><contributor>Brabazon, Dermot</contributor><contributor>Naher, Sumsun</contributor><creatorcontrib>O'Neill, Paul F.</creatorcontrib><creatorcontrib>Kent, Nigel</creatorcontrib><creatorcontrib>Brabazon, Dermot</creatorcontrib><title>Mitigation and control of the overcuring effect in mask projection micro-stereolithography</title><title>AIP conference proceedings</title><description>Mask Projection micro-Stereolithography (MPμSL) is an additive manufacturing technique capable of producing solid parts with micron-scale resolution from a vat of photocurable liquid polymer resin. Although the physical mechanism remains the same, the process differs from traditional laser-galvanometer based stereolithography (SL) in its use of a dynamic mask UV projector, or digital light processor (DLP), which cures each location within each 3D layer at the same time. One area where MPµSL has garnered considerable attention is in the field of microfluidics and Lab-on-a-Chip, where complex multistep microfabrication techniques adopted from the semiconductor industry are still widely used, and where MPµSL offers the ability to fabricate completely encapsulated fluidic channels in a single step and at low cost [1–3]. However, a significant obstacle exists in the prevention of channel blockage due to overcuring of the polymer resin [4, 5]. Overcuring can be attributed to the so-called ‘back side effect’ [2] which occurs during the build process as light from successive layers penetrates into the resin to a depth greater than the layer thickness. This effect is most prevalent in channels or features oriented horizontally (in a parallel plane to that of the build platform). Currently there are two main approaches in controlling the cure depth; 1. the chemical approach, which involves doping the resin material with a chemical light absorber [6–8]; and 2. by improving the system's hardware and optical elements to improve the homogeneity of the light dosage and control the cure depth [9]. Here we investigate a third approach through modification of the 3D CAD file prior to printing to mitigate for UV light leakage from successive build layers. Although used here in conjunction with the MPμSL technique, this approach can be applied to a range of SL techniques to improve printer resolution and enable production of internal features with higher dimensional accuracy.</description><subject>Channels</subject><subject>Cures</subject><subject>Galvanometers</subject><subject>Lithography</subject><subject>Microfluidics</subject><subject>Microprocessors</subject><subject>Optical components</subject><subject>Organic chemistry</subject><subject>Rapid prototyping</subject><subject>Thickness</subject><subject>Ultraviolet radiation</subject><issn>0094-243X</issn><issn>1551-7616</issn><fulltext>true</fulltext><rsrctype>conference_proceeding</rsrctype><creationdate>2017</creationdate><recordtype>conference_proceeding</recordtype><recordid>eNp9kE9LAzEQxYMoWKsHv0HAm7B1Jskmm6MU_0HFi4J4CWk226a2m5pNC_32brXgzdMw8Hsz7z1CLhFGCJLf4KgEqJjQR2SAZYmFkiiPyQBAi4IJ_n5KzrpuAcC0UtWAfDyHHGY2h9hS29bUxTanuKSxoXnuadz65DYptDPqm8a7TENLV7b7pOsUF_2-162CS7Hosk8-LkOex1my6_nunJw0dtn5i8Mckrf7u9fxYzF5eXga304Kx1mVCyeYBSd1jXXvvBQ4Vbbm2qKeIuoKQUumpBUcVKmV8IKjkjUwyZmaAkM-JFe_d3tLXxvfZbOIm9T2Lw1DlCCYLHlPXf9SnQv5J69Zp7CyaWe2MRk0h97Mum7-gxHMvug_Af8GEoxurQ</recordid><startdate>20171016</startdate><enddate>20171016</enddate><creator>O'Neill, Paul F.</creator><creator>Kent, Nigel</creator><creator>Brabazon, Dermot</creator><general>American Institute of Physics</general><scope>8FD</scope><scope>H8D</scope><scope>L7M</scope></search><sort><creationdate>20171016</creationdate><title>Mitigation and control of the overcuring effect in mask projection micro-stereolithography</title><author>O'Neill, Paul F. ; Kent, Nigel ; Brabazon, Dermot</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c328t-c42a0c69d1d008541b7ad39a19b11981096276a43075974e43176d026327b0213</frbrgroupid><rsrctype>conference_proceedings</rsrctype><prefilter>conference_proceedings</prefilter><language>eng</language><creationdate>2017</creationdate><topic>Channels</topic><topic>Cures</topic><topic>Galvanometers</topic><topic>Lithography</topic><topic>Microfluidics</topic><topic>Microprocessors</topic><topic>Optical components</topic><topic>Organic chemistry</topic><topic>Rapid prototyping</topic><topic>Thickness</topic><topic>Ultraviolet radiation</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>O'Neill, Paul F.</creatorcontrib><creatorcontrib>Kent, Nigel</creatorcontrib><creatorcontrib>Brabazon, Dermot</creatorcontrib><collection>Technology Research Database</collection><collection>Aerospace Database</collection><collection>Advanced Technologies Database with Aerospace</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>O'Neill, Paul F.</au><au>Kent, Nigel</au><au>Brabazon, Dermot</au><au>Ahad, Inam Ul</au><au>Brabazon, Dermot</au><au>Naher, Sumsun</au><format>book</format><genre>proceeding</genre><ristype>CONF</ristype><atitle>Mitigation and control of the overcuring effect in mask projection micro-stereolithography</atitle><btitle>AIP conference proceedings</btitle><date>2017-10-16</date><risdate>2017</risdate><volume>1896</volume><issue>1</issue><issn>0094-243X</issn><eissn>1551-7616</eissn><coden>APCPCS</coden><abstract>Mask Projection micro-Stereolithography (MPμSL) is an additive manufacturing technique capable of producing solid parts with micron-scale resolution from a vat of photocurable liquid polymer resin. Although the physical mechanism remains the same, the process differs from traditional laser-galvanometer based stereolithography (SL) in its use of a dynamic mask UV projector, or digital light processor (DLP), which cures each location within each 3D layer at the same time. One area where MPµSL has garnered considerable attention is in the field of microfluidics and Lab-on-a-Chip, where complex multistep microfabrication techniques adopted from the semiconductor industry are still widely used, and where MPµSL offers the ability to fabricate completely encapsulated fluidic channels in a single step and at low cost [1–3]. However, a significant obstacle exists in the prevention of channel blockage due to overcuring of the polymer resin [4, 5]. Overcuring can be attributed to the so-called ‘back side effect’ [2] which occurs during the build process as light from successive layers penetrates into the resin to a depth greater than the layer thickness. This effect is most prevalent in channels or features oriented horizontally (in a parallel plane to that of the build platform). Currently there are two main approaches in controlling the cure depth; 1. the chemical approach, which involves doping the resin material with a chemical light absorber [6–8]; and 2. by improving the system's hardware and optical elements to improve the homogeneity of the light dosage and control the cure depth [9]. Here we investigate a third approach through modification of the 3D CAD file prior to printing to mitigate for UV light leakage from successive build layers. Although used here in conjunction with the MPμSL technique, this approach can be applied to a range of SL techniques to improve printer resolution and enable production of internal features with higher dimensional accuracy.</abstract><cop>Melville</cop><pub>American Institute of Physics</pub><doi>10.1063/1.5008249</doi><tpages>6</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0094-243X |
ispartof | AIP conference proceedings, 2017, Vol.1896 (1) |
issn | 0094-243X 1551-7616 |
language | eng |
recordid | cdi_proquest_journals_2116042653 |
source | American Institute of Physics:Jisc Collections:Transitional Journals Agreement 2021-23 (Reading list) |
subjects | Channels Cures Galvanometers Lithography Microfluidics Microprocessors Optical components Organic chemistry Rapid prototyping Thickness Ultraviolet radiation |
title | Mitigation and control of the overcuring effect in mask projection micro-stereolithography |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T13%3A15%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_scita&rft_val_fmt=info:ofi/fmt:kev:mtx:book&rft.genre=proceeding&rft.atitle=Mitigation%20and%20control%20of%20the%20overcuring%20effect%20in%20mask%20projection%20micro-stereolithography&rft.btitle=AIP%20conference%20proceedings&rft.au=O'Neill,%20Paul%20F.&rft.date=2017-10-16&rft.volume=1896&rft.issue=1&rft.issn=0094-243X&rft.eissn=1551-7616&rft.coden=APCPCS&rft_id=info:doi/10.1063/1.5008249&rft_dat=%3Cproquest_scita%3E2116042653%3C/proquest_scita%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c328t-c42a0c69d1d008541b7ad39a19b11981096276a43075974e43176d026327b0213%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=2116042653&rft_id=info:pmid/&rfr_iscdi=true |