Permeable Ceramic with Three-Fraction Electromelted Corundum Filler and Porcelain Binder
Porous permeable materials are prepared by selecting the grain size composition with electromelted corundum filler and porcelain mix PFL-1 binder. Specimens with an improved set of properties are prepared with addition to the composition of 5 wt.% porcelain binder (above 100% filler) after firing at...
Saved in:
Published in: | Refractories and industrial ceramics 2018-11, Vol.59 (4), p.391-394 |
---|---|
Main Authors: | , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Porous permeable materials are prepared by selecting the grain size composition with electromelted corundum filler and porcelain mix PFL-1 binder. Specimens with an improved set of properties are prepared with addition to the composition of 5 wt.% porcelain binder (above 100% filler) after firing at 1450°C. Specimen ultimate strength in bending is 14.6 MPa, open porosity 44%, and gas permeability coefficient 0.85 μm