Magnesium vapor reduction of complex double compounds of molybdenum with tungsten

The process of obtaining powder of the Mo-W alloy by magnesium vapor reduction of MgWxMo1-xO4 and CaWxMo1-xO4 oxide compounds (x = 0.3) with a residual inert gas pressure of 2-20 kPa in the temperature range 700-800°C was investigated. Argon or helium was used as an inert gas. Powders of Mo-W alloy...

Full description

Saved in:
Bibliographic Details
Published in:Journal of physics. Conference series 2019-12, Vol.1347 (1), p.12128
Main Authors: Kolosov, V N, Miroshnichenko, M N, Prokhorova, T Yu
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The process of obtaining powder of the Mo-W alloy by magnesium vapor reduction of MgWxMo1-xO4 and CaWxMo1-xO4 oxide compounds (x = 0.3) with a residual inert gas pressure of 2-20 kPa in the temperature range 700-800°C was investigated. Argon or helium was used as an inert gas. Powders of Mo-W alloy with a specific surface area of up to 20 m2g-1 were obtained. When both types of compounds were reduced at a residual pressure in the reactor of more than 5 kPa, spatial separation of the reaction products was observed with removal of magnesium oxide from the reaction zone.
ISSN:1742-6588
1742-6596
DOI:10.1088/1742-6596/1347/1/012128