Thermoelectric Properties of Cd3As2 + n mol % MnAs (n = 10, 20, 30, 44.7) at High Pressures

— The results of studying the thermal emf of composites Cd 3 As 2 + n mol % MnAs ( n = 10, 20, 30, 44.7) at high pressures up to 50 GPa are presented. In the pressure ranges of P = 28–35 GPa ( n = 10, 20), 20–35 GPa ( n = 30), and 30–35 GPa ( n = 44.7), all the materials studied exhibit specific fea...

Full description

Saved in:
Bibliographic Details
Published in:Surface investigation, x-ray, synchrotron and neutron techniques x-ray, synchrotron and neutron techniques, 2022-06, Vol.16 (3), p.390-396
Main Authors: Saypulaeva, L. A., Alibekov, A. G., Melnikova, N. V., Sukhanova, G. V., Tebenkov, A. V., Babushkin, A. N., Gadzhialiev, M. M., Zakhvalinskii, V. S., Ril, A. I., Marenkin, S. F.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:— The results of studying the thermal emf of composites Cd 3 As 2 + n mol % MnAs ( n = 10, 20, 30, 44.7) at high pressures up to 50 GPa are presented. In the pressure ranges of P = 28–35 GPa ( n = 10, 20), 20–35 GPa ( n = 30), and 30–35 GPa ( n = 44.7), all the materials studied exhibit specific features in the behavior of the thermal emf S ( P ) (extrema, inflection points on the curves or hysteresis). At a pressure exceeding 40 GPa, the thermal emf changes weakly or barely changes with an increase and a subsequent decrease in pressure.
ISSN:1027-4510
1819-7094
DOI:10.1134/S1027451022020197