SummaryThe polyamide 6 (PA6)/K resin (K) blends of some kinds of compositions have been prepared by extrusion. During the process of tensile testing, we found that the PA6/K blend with 10% PA6 has the usual stress-strain behavior, and that the samples obtained with 30% and 50% PA6 show apparently do...

Full description

Saved in:
Bibliographic Details
Published in:Polymer bulletin (Berlin, Germany) Germany), 2006-07, Vol.57 (3), p.359-367
Main Authors: Jing, Bo, Dai, Wenli, Cao, Qi, Liu, Pengsheng
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:SummaryThe polyamide 6 (PA6)/K resin (K) blends of some kinds of compositions have been prepared by extrusion. During the process of tensile testing, we found that the PA6/K blend with 10% PA6 has the usual stress-strain behavior, and that the samples obtained with 30% and 50% PA6 show apparently double yielding behavior, while the PA6/PS blend does not show the double yielding phenomenon at all same mass ratio. Considering the microscopic morphology study and results of mechanical properties of the PA6/K blends, the first yield point which occurs at the lower tensile stress might be caused by the deformation of the K resin matrix, and the second one may be correlated to the permanent plastic deformation of the entanglement of PA6 chains and PB segments within chains of K resin.
ISSN:0170-0839
1436-2449
DOI:10.1007/s00289-006-0562-y