Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions

AbstractThe macroscopic physical and mechanical behavior, mesocosmic pore size distribution, and microscopic particle morphology of polyurethane concrete (PUC) during freeze–thaw conditions are thoroughly examined in this research. The results reveal that as the number of freeze–thaw cycles (F-T cyc...

Full description

Saved in:
Bibliographic Details
Published in:Journal of materials in civil engineering 2024-11, Vol.36 (11)
Main Authors: Wu, Yuxuan, Xu, Wenyuan, Yu, Tianlai, Ji, Yongcheng
Format: Article
Language:English
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by
cites
container_end_page
container_issue 11
container_start_page
container_title Journal of materials in civil engineering
container_volume 36
creator Wu, Yuxuan
Xu, Wenyuan
Yu, Tianlai
Ji, Yongcheng
description AbstractThe macroscopic physical and mechanical behavior, mesocosmic pore size distribution, and microscopic particle morphology of polyurethane concrete (PUC) during freeze–thaw conditions are thoroughly examined in this research. The results reveal that as the number of freeze–thaw cycles (F-T cycles) increases, the P-wave velocity of PUC drops constantly, the peak shear strength reduces gradually, but the porosity increases. A four-peak exponential function can be used to describe the pore dispersion features of PUC. With the increase in the number of F-T cycles, PUC showed an increasing trend in all characteristic pore radii, but only the volume fraction of macropores increased. The compressive and shear strength of PUC were positively correlated with the volume fraction of nanopores and micropores and negatively correlated with the volume fraction of macropores. It was proved that the macroporous content is the main reason for the decrease in the mechanical properties of PUC. The fractal dimension of PUC decreases with the increase in the number of F-T cycles, indicating that the complexity of the PUC pore structure decreases after F-T cycles. At the micro-meso-macro scale, the damage progression of PUC under freeze–thaw conditions demonstrates a gradual and mutually feeding connection. The damage evolution process can be broadly divided into three stages, beginning with the formation of micropores in the polyurethane agglomeration, progressing to the gradual germination and expansion of cracks in the polyurethane agglomeration, and finally to the connected sum expansion of cracks between the polyurethane agglomeration and the aggregates, resulting in significant deterioration of the macromechanical properties of PUC.
doi_str_mv 10.1061/JMCEE7.MTENG-18003
format article
fullrecord <record><control><sourceid>proquest_asce_</sourceid><recordid>TN_cdi_proquest_journals_3097028803</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3097028803</sourcerecordid><originalsourceid>FETCH-LOGICAL-a153t-8b8367a10c516d5880ef6d23b5bfd3c213f3236ec24b077e44f249c6c9cc48493</originalsourceid><addsrcrecordid>eNpFkMFOg0AQhjdGE2v1BTxt4pl2l9ld4GiQVk1RE-uZLMtgaSgoCzX15Dv4hj6J0Jp4msn8X_5JPkIuOZtwpvj0Pg6jyJvEy-hh7nCfMTgiIx4IcKQEOCYj5geBw6Xip-TM2jXrCSbYiKzjrmwLa3SJ9Lntsh2tc9qukN7ojX5FGm3rsmuLuqIxmpWuCrsZiKe63HUNtv0FaVhXpt-RdlWGDZ01iJ_48_W9XOmPIcyKocCek5NclxYv_uaYvMyiZXjrLB7nd-H1wtFcQuv4qQ_K05wZyVUmfZ9hrjIXUpnmGRiXQw4uKDSuSJnnoRC5KwKjTGCM8EUAY3J16H1r6vcObZus666p-pcJsMBjbl8JPTU9UNoa_Cc4SwahyUFoshea7IXCLxcsav4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>3097028803</pqid></control><display><type>article</type><title>Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions</title><source>ASCE Library</source><creator>Wu, Yuxuan ; Xu, Wenyuan ; Yu, Tianlai ; Ji, Yongcheng</creator><creatorcontrib>Wu, Yuxuan ; Xu, Wenyuan ; Yu, Tianlai ; Ji, Yongcheng</creatorcontrib><description>AbstractThe macroscopic physical and mechanical behavior, mesocosmic pore size distribution, and microscopic particle morphology of polyurethane concrete (PUC) during freeze–thaw conditions are thoroughly examined in this research. The results reveal that as the number of freeze–thaw cycles (F-T cycles) increases, the P-wave velocity of PUC drops constantly, the peak shear strength reduces gradually, but the porosity increases. A four-peak exponential function can be used to describe the pore dispersion features of PUC. With the increase in the number of F-T cycles, PUC showed an increasing trend in all characteristic pore radii, but only the volume fraction of macropores increased. The compressive and shear strength of PUC were positively correlated with the volume fraction of nanopores and micropores and negatively correlated with the volume fraction of macropores. It was proved that the macroporous content is the main reason for the decrease in the mechanical properties of PUC. The fractal dimension of PUC decreases with the increase in the number of F-T cycles, indicating that the complexity of the PUC pore structure decreases after F-T cycles. At the micro-meso-macro scale, the damage progression of PUC under freeze–thaw conditions demonstrates a gradual and mutually feeding connection. The damage evolution process can be broadly divided into three stages, beginning with the formation of micropores in the polyurethane agglomeration, progressing to the gradual germination and expansion of cracks in the polyurethane agglomeration, and finally to the connected sum expansion of cracks between the polyurethane agglomeration and the aggregates, resulting in significant deterioration of the macromechanical properties of PUC.</description><identifier>ISSN: 0899-1561</identifier><identifier>EISSN: 1943-5533</identifier><identifier>DOI: 10.1061/JMCEE7.MTENG-18003</identifier><language>eng</language><publisher>New York: American Society of Civil Engineers</publisher><subject>Agglomeration ; Compressive strength ; Damage ; Exponential functions ; Fractal geometry ; Freeze thaw cycles ; Germination ; Mechanical properties ; P waves ; Polyurethane resins ; Pore size distribution ; Porosity ; Shear strength ; Technical Papers ; Wave velocity</subject><ispartof>Journal of materials in civil engineering, 2024-11, Vol.36 (11)</ispartof><rights>2024 American Society of Civil Engineers</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttp://ascelibrary.org/doi/pdf/10.1061/JMCEE7.MTENG-18003$$EPDF$$P50$$Gasce$$H</linktopdf><linktohtml>$$Uhttp://ascelibrary.org/doi/abs/10.1061/JMCEE7.MTENG-18003$$EHTML$$P50$$Gasce$$H</linktohtml><link.rule.ids>314,780,784,10068,27924,27925,76191,76199</link.rule.ids></links><search><creatorcontrib>Wu, Yuxuan</creatorcontrib><creatorcontrib>Xu, Wenyuan</creatorcontrib><creatorcontrib>Yu, Tianlai</creatorcontrib><creatorcontrib>Ji, Yongcheng</creatorcontrib><title>Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions</title><title>Journal of materials in civil engineering</title><description>AbstractThe macroscopic physical and mechanical behavior, mesocosmic pore size distribution, and microscopic particle morphology of polyurethane concrete (PUC) during freeze–thaw conditions are thoroughly examined in this research. The results reveal that as the number of freeze–thaw cycles (F-T cycles) increases, the P-wave velocity of PUC drops constantly, the peak shear strength reduces gradually, but the porosity increases. A four-peak exponential function can be used to describe the pore dispersion features of PUC. With the increase in the number of F-T cycles, PUC showed an increasing trend in all characteristic pore radii, but only the volume fraction of macropores increased. The compressive and shear strength of PUC were positively correlated with the volume fraction of nanopores and micropores and negatively correlated with the volume fraction of macropores. It was proved that the macroporous content is the main reason for the decrease in the mechanical properties of PUC. The fractal dimension of PUC decreases with the increase in the number of F-T cycles, indicating that the complexity of the PUC pore structure decreases after F-T cycles. At the micro-meso-macro scale, the damage progression of PUC under freeze–thaw conditions demonstrates a gradual and mutually feeding connection. The damage evolution process can be broadly divided into three stages, beginning with the formation of micropores in the polyurethane agglomeration, progressing to the gradual germination and expansion of cracks in the polyurethane agglomeration, and finally to the connected sum expansion of cracks between the polyurethane agglomeration and the aggregates, resulting in significant deterioration of the macromechanical properties of PUC.</description><subject>Agglomeration</subject><subject>Compressive strength</subject><subject>Damage</subject><subject>Exponential functions</subject><subject>Fractal geometry</subject><subject>Freeze thaw cycles</subject><subject>Germination</subject><subject>Mechanical properties</subject><subject>P waves</subject><subject>Polyurethane resins</subject><subject>Pore size distribution</subject><subject>Porosity</subject><subject>Shear strength</subject><subject>Technical Papers</subject><subject>Wave velocity</subject><issn>0899-1561</issn><issn>1943-5533</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2024</creationdate><recordtype>article</recordtype><recordid>eNpFkMFOg0AQhjdGE2v1BTxt4pl2l9ld4GiQVk1RE-uZLMtgaSgoCzX15Dv4hj6J0Jp4msn8X_5JPkIuOZtwpvj0Pg6jyJvEy-hh7nCfMTgiIx4IcKQEOCYj5geBw6Xip-TM2jXrCSbYiKzjrmwLa3SJ9Lntsh2tc9qukN7ojX5FGm3rsmuLuqIxmpWuCrsZiKe63HUNtv0FaVhXpt-RdlWGDZ01iJ_48_W9XOmPIcyKocCek5NclxYv_uaYvMyiZXjrLB7nd-H1wtFcQuv4qQ_K05wZyVUmfZ9hrjIXUpnmGRiXQw4uKDSuSJnnoRC5KwKjTGCM8EUAY3J16H1r6vcObZus666p-pcJsMBjbl8JPTU9UNoa_Cc4SwahyUFoshea7IXCLxcsav4</recordid><startdate>20241101</startdate><enddate>20241101</enddate><creator>Wu, Yuxuan</creator><creator>Xu, Wenyuan</creator><creator>Yu, Tianlai</creator><creator>Ji, Yongcheng</creator><general>American Society of Civil Engineers</general><scope>8FD</scope><scope>FR3</scope><scope>KR7</scope></search><sort><creationdate>20241101</creationdate><title>Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions</title><author>Wu, Yuxuan ; Xu, Wenyuan ; Yu, Tianlai ; Ji, Yongcheng</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a153t-8b8367a10c516d5880ef6d23b5bfd3c213f3236ec24b077e44f249c6c9cc48493</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2024</creationdate><topic>Agglomeration</topic><topic>Compressive strength</topic><topic>Damage</topic><topic>Exponential functions</topic><topic>Fractal geometry</topic><topic>Freeze thaw cycles</topic><topic>Germination</topic><topic>Mechanical properties</topic><topic>P waves</topic><topic>Polyurethane resins</topic><topic>Pore size distribution</topic><topic>Porosity</topic><topic>Shear strength</topic><topic>Technical Papers</topic><topic>Wave velocity</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Wu, Yuxuan</creatorcontrib><creatorcontrib>Xu, Wenyuan</creatorcontrib><creatorcontrib>Yu, Tianlai</creatorcontrib><creatorcontrib>Ji, Yongcheng</creatorcontrib><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>Journal of materials in civil engineering</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Wu, Yuxuan</au><au>Xu, Wenyuan</au><au>Yu, Tianlai</au><au>Ji, Yongcheng</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions</atitle><jtitle>Journal of materials in civil engineering</jtitle><date>2024-11-01</date><risdate>2024</risdate><volume>36</volume><issue>11</issue><issn>0899-1561</issn><eissn>1943-5533</eissn><abstract>AbstractThe macroscopic physical and mechanical behavior, mesocosmic pore size distribution, and microscopic particle morphology of polyurethane concrete (PUC) during freeze–thaw conditions are thoroughly examined in this research. The results reveal that as the number of freeze–thaw cycles (F-T cycles) increases, the P-wave velocity of PUC drops constantly, the peak shear strength reduces gradually, but the porosity increases. A four-peak exponential function can be used to describe the pore dispersion features of PUC. With the increase in the number of F-T cycles, PUC showed an increasing trend in all characteristic pore radii, but only the volume fraction of macropores increased. The compressive and shear strength of PUC were positively correlated with the volume fraction of nanopores and micropores and negatively correlated with the volume fraction of macropores. It was proved that the macroporous content is the main reason for the decrease in the mechanical properties of PUC. The fractal dimension of PUC decreases with the increase in the number of F-T cycles, indicating that the complexity of the PUC pore structure decreases after F-T cycles. At the micro-meso-macro scale, the damage progression of PUC under freeze–thaw conditions demonstrates a gradual and mutually feeding connection. The damage evolution process can be broadly divided into three stages, beginning with the formation of micropores in the polyurethane agglomeration, progressing to the gradual germination and expansion of cracks in the polyurethane agglomeration, and finally to the connected sum expansion of cracks between the polyurethane agglomeration and the aggregates, resulting in significant deterioration of the macromechanical properties of PUC.</abstract><cop>New York</cop><pub>American Society of Civil Engineers</pub><doi>10.1061/JMCEE7.MTENG-18003</doi></addata></record>
fulltext fulltext
identifier ISSN: 0899-1561
ispartof Journal of materials in civil engineering, 2024-11, Vol.36 (11)
issn 0899-1561
1943-5533
language eng
recordid cdi_proquest_journals_3097028803
source ASCE Library
subjects Agglomeration
Compressive strength
Damage
Exponential functions
Fractal geometry
Freeze thaw cycles
Germination
Mechanical properties
P waves
Polyurethane resins
Pore size distribution
Porosity
Shear strength
Technical Papers
Wave velocity
title Multiscale Study of the Damage Evolution Mechanism of Polyurethane Concrete under Freeze–Thaw Conditions
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T03%3A06%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_asce_&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Multiscale%20Study%20of%20the%20Damage%20Evolution%20Mechanism%20of%20Polyurethane%20Concrete%20under%20Freeze%E2%80%93Thaw%20Conditions&rft.jtitle=Journal%20of%20materials%20in%20civil%20engineering&rft.au=Wu,%20Yuxuan&rft.date=2024-11-01&rft.volume=36&rft.issue=11&rft.issn=0899-1561&rft.eissn=1943-5533&rft_id=info:doi/10.1061/JMCEE7.MTENG-18003&rft_dat=%3Cproquest_asce_%3E3097028803%3C/proquest_asce_%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-a153t-8b8367a10c516d5880ef6d23b5bfd3c213f3236ec24b077e44f249c6c9cc48493%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=3097028803&rft_id=info:pmid/&rfr_iscdi=true