UV photodetector behavior of 2D ZnO plates prepared by electrochemical deposition

► ZnO with 2D hexagonal structure was successfully prepared using electrochemical method. ► The study found the maximum response of the UV photodetector was in the range of 300–350nm. ► The internal gain of the ZnO photodetector was 2.7 at low UV intensity. Zinc oxide (ZnO) with 2D hexagonal structu...

Full description

Saved in:
Bibliographic Details
Published in:Superlattices and microstructures 2012-06, Vol.51 (6), p.765-771
Main Authors: Al-Hardan, N.H., Abdullah, M.J., Ahmed, N.M., Yam, F.K., Abdul Aziz, A.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:► ZnO with 2D hexagonal structure was successfully prepared using electrochemical method. ► The study found the maximum response of the UV photodetector was in the range of 300–350nm. ► The internal gain of the ZnO photodetector was 2.7 at low UV intensity. Zinc oxide (ZnO) with 2D hexagonal structure was successfully prepared using electrochemical deposition (ECD) method on a quartz substrate pre-coated with indium-doped ZnO layer. The X-ray diffraction of the prepared sample confirmed that the hexagonal structure had a dominant c-axis orientation. The scanning electron microscopy revealed the 2D hexagonal structure of the prepared ZnO. An ultraviolet (UV) photodetector based on the prepared ZnO was fabricated using two parallel palladium thin films as electrodes. The maximum response of the UV photodetector was in the range of 300–350nm wavelength. The internal gain of the ZnO photodetector was 2.7 at low UV intensity. The response and the recovery times were estimated to be 26 and 11s, respectively.
ISSN:0749-6036
1096-3677
DOI:10.1016/j.spmi.2012.03.030