Release of metals from synthetic Cr-goethites under acidic and reductive conditions: Effect of aging and composition
The dissolution mechanism of pure and Cr-substituted, synthetic goethites with different aging times, as well as the changes in morphology, crystallinity and structural changes, were investigated. The Cr-goethites were obtained by synthesizing goethite in solutions that contained different concentra...
Saved in:
Published in: | Applied clay science 2012-04, Vol.58, p.88-95 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The dissolution mechanism of pure and Cr-substituted, synthetic goethites with different aging times, as well as the changes in morphology, crystallinity and structural changes, were investigated. The Cr-goethites were obtained by synthesizing goethite in solutions that contained different concentrations of Cr(III) ions. The obtained suspensions were aged in the parent solutions for different time spans. Two samples of pure goethites, prepared using different KOH concentrations, were also studied for comparative purposes.
Chemical analyses showed that Cr-for-Fe substitution was greatest in samples aged for longer time. Rietveld simulation of XRD powder data indicated that the unit cell parameters of pure goethite increased for samples prepared at a higher KOH concentration, and decreased with Cr-incorporation. Simulation also showed that the mean coherence path dimension (MCP), or crystallite size, in the direction perpendicular to crystal plane (110), did not change much in the samples, whereas the crystallite size in the direction parallel to crystal plane (110) increased with Cr-content, KOH concentration and aging time. The obtained MCP values indicate an increasing elongated form in the domains.
Chromium substituted goethites presented a good capacity for immobilizating Cr when the dissolution rates were studied in 3.98M HCl, 0.10M oxalic acid (H2Oxal), and reductive media (H2Oxal/Fe(II)). The shape of the f vs. t profile, where f stands for the fraction of Fe dissolved (dissolved Fe mass/total Fe mass) and t refers to the dissolution time, follows a contracting bidimensional model, and when dissolved in similar acid concentrations, the reactivity follows the trend HCl |
---|---|