Leaching of Calcareous Bornite Ore in Ammoniacal Solution Containing Ammonium Persulfate
The leaching process of copper from calcareous bornite ore using ammonium persulfate as an oxidant in ammoniacal solution was investigated. The effects of stirring speed, temperature, initial concentration of ammonia and ammonium persulfate, and liquid-to-solid (L/S) ratio on the extraction percenta...
Saved in:
Published in: | Metallurgical and materials transactions. B, Process metallurgy and materials processing science Process metallurgy and materials processing science, 2014-12, Vol.45 (6), p.2027-2032 |
---|---|
Main Authors: | , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The leaching process of copper from calcareous bornite ore using ammonium persulfate as an oxidant in ammoniacal solution was investigated. The effects of stirring speed, temperature, initial concentration of ammonia and ammonium persulfate, and liquid-to-solid (L/S) ratio on the extraction percentage of copper from bornite ore were studied. The results show that the optimum leaching conditions for bornite ore with a maximum extraction of copper 88.9 pct are temperature 313.15 K (40 °C), reaction time 4 hours, stirring speed 600 r
/
min, L/S ratio 7/1 cm
3
/g, initial concentration of ammonia 2.0 mol/dm
3
, and ammonium persulfate 3.0 mol/dm
3
. |
---|---|
ISSN: | 1073-5615 1543-1916 |
DOI: | 10.1007/s11663-014-0139-3 |