TiSiN Coatings for Improved Bond Strength of CoCr Alloy to Dental Ceramic

In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and cor...

Full description

Saved in:
Bibliographic Details
Published in:Key engineering materials 2014-01, Vol.587, p.275-281
Main Authors: Colease, Gabriel, Cotrut, Mihai Cosmin, Vladescu, Alina, Vrânceanu, Maria-Diana, Dinu, Mihaela, Braic, Viorel, Baciu, Florin, Tarcolea, Mihai, Vitelaru, Catalin, Braic, Mariana
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In this work, TiSiN coatings were selected to improve the adhesion between dental ceramic and CoCr substrate. The coatings were prepared by the cathodic arc technique in N2 reactive atmosphere, at different bias voltages, and analyzed for elemental composition, surface roughness, wettability and corrosion resistance in Fusayama Meyer artificial saliva. After the coating deposition, low-fusing dental ceramic film was fired on coated alloy, using a dental furnace. The bond strength of these specimens was tested using a 3-point bending test.
ISSN:1013-9826
1662-9795
1662-9795
DOI:10.4028/www.scientific.net/KEM.587.275