Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics
Using BaO–B2O3–SiO2 (BBS)‐based frit as sintering aid, the K0.49Na0.51NbO3 (KNN) + x wt% BBS (x = 1.0, 1.5, 2.0 and 2.5) lead‐free piezoelectric ceramics were successfully fabricated by solid‐state reaction method under low‐sintering temperature of 1000°C. The effect of BBS frit doping amount on the...
Saved in:
Published in: | International journal of applied ceramic technology 2013-09, Vol.10 (5), p.866-872 |
---|---|
Main Authors: | , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | cdi_FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513 |
---|---|
cites | cdi_FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513 |
container_end_page | 872 |
container_issue | 5 |
container_start_page | 866 |
container_title | International journal of applied ceramic technology |
container_volume | 10 |
creator | Li, Yue-Ming Shen, Zong-Yang Li, Run-Run Wang, Zhu-Mei Hong, Yan Liao, Run-Hua |
description | Using BaO–B2O3–SiO2 (BBS)‐based frit as sintering aid, the K0.49Na0.51NbO3 (KNN) + x wt% BBS (x = 1.0, 1.5, 2.0 and 2.5) lead‐free piezoelectric ceramics were successfully fabricated by solid‐state reaction method under low‐sintering temperature of 1000°C. The effect of BBS frit doping amount on the structure and electrical properties of the ceramics was investigated. The KNN ceramics with 1.5 wt% BBS frit showed optimal properties as follows: piezoelectric constant d33 = 108 pC/N, planar electromechanical coupling coefficient kp = 41%, mechanical quality factor Qm = 225, relative dielectric constant εr = 410, dielectric loss tanδ = 0.57% and Curie temperature Tc = 400°C. This ceramic sample should be a good lead‐free candidate for actuators or high temperature sensors application due to its ultra‐low tanδ, relatively high Qm and Tc. |
doi_str_mv | 10.1111/j.1744-7402.2012.02794.x |
format | article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1692364381</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>1692364381</sourcerecordid><originalsourceid>FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513</originalsourceid><addsrcrecordid>eNqNkU9v0zAYhyMEEmPwHSxx4ZLiv7FzQmvVboOqTKzAbpZjvwaXNCl2qnV8epwV7cCpvtiyn98j-f0VBSJ4QvJ6v5kQyXkpOaYTigmdYCprPjk8K86eHp7ns-BVKTi9e1m8SmmDMeOMVWdFnHsPdkC9R9PpbTk1CRxaxJBvOjT8BLTs79EatjuIZthHQLehGyCG7gcynUPzNodjsKZFN7HP0BAgjbJPqxVagnHlIgKgmwB_epsV22DT6-KFN22CN__28-LrYr6eXZXLz5fXs4tlaQXDvPSNN9g3xCjKwTEnPOO0YYY2jaSNU40VNfY1F54qcNL72lmrvJIgnGOCsPPi3dG7i_3vPaRBb0Oy0Lamg36fNKlqyirO1Akor_O46jzDE1CuJFGMi4y-_Q_d9PvY5T9rIkR2qpqxTKkjZWOfUgSvdzFsTXzQBOuxYr3RY5N6bFKPFevHivUhRz8co_ehhYeTc_r648Xs8ZwN5dEQ0gCHJ4OJv3QlmRT6--pSX8nF3TexXusv7C9qq7tp</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1551498933</pqid></control><display><type>article</type><title>Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics</title><source>Wiley</source><creator>Li, Yue-Ming ; Shen, Zong-Yang ; Li, Run-Run ; Wang, Zhu-Mei ; Hong, Yan ; Liao, Run-Hua</creator><creatorcontrib>Li, Yue-Ming ; Shen, Zong-Yang ; Li, Run-Run ; Wang, Zhu-Mei ; Hong, Yan ; Liao, Run-Hua</creatorcontrib><description>Using BaO–B2O3–SiO2 (BBS)‐based frit as sintering aid, the K0.49Na0.51NbO3 (KNN) + x wt% BBS (x = 1.0, 1.5, 2.0 and 2.5) lead‐free piezoelectric ceramics were successfully fabricated by solid‐state reaction method under low‐sintering temperature of 1000°C. The effect of BBS frit doping amount on the structure and electrical properties of the ceramics was investigated. The KNN ceramics with 1.5 wt% BBS frit showed optimal properties as follows: piezoelectric constant d33 = 108 pC/N, planar electromechanical coupling coefficient kp = 41%, mechanical quality factor Qm = 225, relative dielectric constant εr = 410, dielectric loss tanδ = 0.57% and Curie temperature Tc = 400°C. This ceramic sample should be a good lead‐free candidate for actuators or high temperature sensors application due to its ultra‐low tanδ, relatively high Qm and Tc.</description><identifier>ISSN: 1546-542X</identifier><identifier>EISSN: 1744-7402</identifier><identifier>DOI: 10.1111/j.1744-7402.2012.02794.x</identifier><language>eng</language><publisher>Malden: Blackwell Publishing Ltd</publisher><subject>Actuators ; Ceramics ; Curie temperature ; Dielectric loss ; Electrical properties ; Frit ; Lead free ; Piezoelectric ceramics ; Sintering ; Tangents</subject><ispartof>International journal of applied ceramic technology, 2013-09, Vol.10 (5), p.866-872</ispartof><rights>2012 The American Ceramic Society</rights><rights>Copyright © 2013 American Ceramic Society</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513</citedby><cites>FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27922,27923</link.rule.ids></links><search><creatorcontrib>Li, Yue-Ming</creatorcontrib><creatorcontrib>Shen, Zong-Yang</creatorcontrib><creatorcontrib>Li, Run-Run</creatorcontrib><creatorcontrib>Wang, Zhu-Mei</creatorcontrib><creatorcontrib>Hong, Yan</creatorcontrib><creatorcontrib>Liao, Run-Hua</creatorcontrib><title>Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics</title><title>International journal of applied ceramic technology</title><addtitle>Int. J. Appl. Ceram. Technol</addtitle><description>Using BaO–B2O3–SiO2 (BBS)‐based frit as sintering aid, the K0.49Na0.51NbO3 (KNN) + x wt% BBS (x = 1.0, 1.5, 2.0 and 2.5) lead‐free piezoelectric ceramics were successfully fabricated by solid‐state reaction method under low‐sintering temperature of 1000°C. The effect of BBS frit doping amount on the structure and electrical properties of the ceramics was investigated. The KNN ceramics with 1.5 wt% BBS frit showed optimal properties as follows: piezoelectric constant d33 = 108 pC/N, planar electromechanical coupling coefficient kp = 41%, mechanical quality factor Qm = 225, relative dielectric constant εr = 410, dielectric loss tanδ = 0.57% and Curie temperature Tc = 400°C. This ceramic sample should be a good lead‐free candidate for actuators or high temperature sensors application due to its ultra‐low tanδ, relatively high Qm and Tc.</description><subject>Actuators</subject><subject>Ceramics</subject><subject>Curie temperature</subject><subject>Dielectric loss</subject><subject>Electrical properties</subject><subject>Frit</subject><subject>Lead free</subject><subject>Piezoelectric ceramics</subject><subject>Sintering</subject><subject>Tangents</subject><issn>1546-542X</issn><issn>1744-7402</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2013</creationdate><recordtype>article</recordtype><recordid>eNqNkU9v0zAYhyMEEmPwHSxx4ZLiv7FzQmvVboOqTKzAbpZjvwaXNCl2qnV8epwV7cCpvtiyn98j-f0VBSJ4QvJ6v5kQyXkpOaYTigmdYCprPjk8K86eHp7ns-BVKTi9e1m8SmmDMeOMVWdFnHsPdkC9R9PpbTk1CRxaxJBvOjT8BLTs79EatjuIZthHQLehGyCG7gcynUPzNodjsKZFN7HP0BAgjbJPqxVagnHlIgKgmwB_epsV22DT6-KFN22CN__28-LrYr6eXZXLz5fXs4tlaQXDvPSNN9g3xCjKwTEnPOO0YYY2jaSNU40VNfY1F54qcNL72lmrvJIgnGOCsPPi3dG7i_3vPaRBb0Oy0Lamg36fNKlqyirO1Akor_O46jzDE1CuJFGMi4y-_Q_d9PvY5T9rIkR2qpqxTKkjZWOfUgSvdzFsTXzQBOuxYr3RY5N6bFKPFevHivUhRz8co_ehhYeTc_r648Xs8ZwN5dEQ0gCHJ4OJv3QlmRT6--pSX8nF3TexXusv7C9qq7tp</recordid><startdate>201309</startdate><enddate>201309</enddate><creator>Li, Yue-Ming</creator><creator>Shen, Zong-Yang</creator><creator>Li, Run-Run</creator><creator>Wang, Zhu-Mei</creator><creator>Hong, Yan</creator><creator>Liao, Run-Hua</creator><general>Blackwell Publishing Ltd</general><general>Wiley Subscription Services, Inc</general><scope>BSCLL</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope><scope>8BQ</scope></search><sort><creationdate>201309</creationdate><title>Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics</title><author>Li, Yue-Ming ; Shen, Zong-Yang ; Li, Run-Run ; Wang, Zhu-Mei ; Hong, Yan ; Liao, Run-Hua</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2013</creationdate><topic>Actuators</topic><topic>Ceramics</topic><topic>Curie temperature</topic><topic>Dielectric loss</topic><topic>Electrical properties</topic><topic>Frit</topic><topic>Lead free</topic><topic>Piezoelectric ceramics</topic><topic>Sintering</topic><topic>Tangents</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Li, Yue-Ming</creatorcontrib><creatorcontrib>Shen, Zong-Yang</creatorcontrib><creatorcontrib>Li, Run-Run</creatorcontrib><creatorcontrib>Wang, Zhu-Mei</creatorcontrib><creatorcontrib>Hong, Yan</creatorcontrib><creatorcontrib>Liao, Run-Hua</creatorcontrib><collection>Istex</collection><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>METADEX</collection><jtitle>International journal of applied ceramic technology</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Li, Yue-Ming</au><au>Shen, Zong-Yang</au><au>Li, Run-Run</au><au>Wang, Zhu-Mei</au><au>Hong, Yan</au><au>Liao, Run-Hua</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics</atitle><jtitle>International journal of applied ceramic technology</jtitle><addtitle>Int. J. Appl. Ceram. Technol</addtitle><date>2013-09</date><risdate>2013</risdate><volume>10</volume><issue>5</issue><spage>866</spage><epage>872</epage><pages>866-872</pages><issn>1546-542X</issn><eissn>1744-7402</eissn><abstract>Using BaO–B2O3–SiO2 (BBS)‐based frit as sintering aid, the K0.49Na0.51NbO3 (KNN) + x wt% BBS (x = 1.0, 1.5, 2.0 and 2.5) lead‐free piezoelectric ceramics were successfully fabricated by solid‐state reaction method under low‐sintering temperature of 1000°C. The effect of BBS frit doping amount on the structure and electrical properties of the ceramics was investigated. The KNN ceramics with 1.5 wt% BBS frit showed optimal properties as follows: piezoelectric constant d33 = 108 pC/N, planar electromechanical coupling coefficient kp = 41%, mechanical quality factor Qm = 225, relative dielectric constant εr = 410, dielectric loss tanδ = 0.57% and Curie temperature Tc = 400°C. This ceramic sample should be a good lead‐free candidate for actuators or high temperature sensors application due to its ultra‐low tanδ, relatively high Qm and Tc.</abstract><cop>Malden</cop><pub>Blackwell Publishing Ltd</pub><doi>10.1111/j.1744-7402.2012.02794.x</doi><tpages>7</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1546-542X |
ispartof | International journal of applied ceramic technology, 2013-09, Vol.10 (5), p.866-872 |
issn | 1546-542X 1744-7402 |
language | eng |
recordid | cdi_proquest_miscellaneous_1692364381 |
source | Wiley |
subjects | Actuators Ceramics Curie temperature Dielectric loss Electrical properties Frit Lead free Piezoelectric ceramics Sintering Tangents |
title | Effect of BBS-Based Frit on the Low Temperature Sintering and Electrical Properties of KNN Lead-Free Piezoceramics |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T11%3A53%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20BBS-Based%20Frit%20on%20the%20Low%20Temperature%20Sintering%20and%20Electrical%20Properties%20of%20KNN%20Lead-Free%20Piezoceramics&rft.jtitle=International%20journal%20of%20applied%20ceramic%20technology&rft.au=Li,%20Yue-Ming&rft.date=2013-09&rft.volume=10&rft.issue=5&rft.spage=866&rft.epage=872&rft.pages=866-872&rft.issn=1546-542X&rft.eissn=1744-7402&rft_id=info:doi/10.1111/j.1744-7402.2012.02794.x&rft_dat=%3Cproquest_cross%3E1692364381%3C/proquest_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c5304-fbfa0fb1a824ed3d5f342b3a2bb72bd8bc590f945f28ed7ff9dcc8f87e5dd3513%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=1551498933&rft_id=info:pmid/&rfr_iscdi=true |