Loading…
Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill
Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zon...
Saved in:
Published in: | Powder metallurgy and metal ceramics 2016-09, Vol.55 (5-6), p.251-258 |
---|---|
Main Authors: | , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | cdi_FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703 |
---|---|
cites | cdi_FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703 |
container_end_page | 258 |
container_issue | 5-6 |
container_start_page | 251 |
container_title | Powder metallurgy and metal ceramics |
container_volume | 55 |
creator | Saviak, M. P. Mel’nik, O. B. Uvarova, I. V. Kotko, A. V. Udovik, O. O. |
description | Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zone. At the initial stage of grinding, texturing of titanium occurs and the titanium lattice cell increases in volume, thus inducing internal stresses. Based on these data, it is suggested that the introduction of carbon into the strained titanium particles leads to stacking faults in the titanium hcp lattice, acting as nuclei of fcc titanium carbide in the titanium sites fragmented. Single-crystal TiC 10–20 nm nanoparticles are formed in these sites. The length of titanium–carbon contacts naturally increases with grinding time, giving rise to more nuclei of the new fcc phase. This promotes a mechanically induced self-propagating reaction. The heat generated in the reaction contributes to the sintering of titanium carbide nanoparticles. This results in the formation of particle aggregates 0.1–0.5 μm in size. |
doi_str_mv | 10.1007/s11106-016-9800-5 |
format | article |
fullrecord | <record><control><sourceid>gale_proqu</sourceid><recordid>TN_cdi_proquest_miscellaneous_1855371243</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><galeid>A470683648</galeid><sourcerecordid>A470683648</sourcerecordid><originalsourceid>FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703</originalsourceid><addsrcrecordid>eNp9kU1vFDEMhkeISpSWH8AtRy4p9nwks8eyogWpQA_lHCUez5JqJlmSmUP765tlkLihHBzF72PHfqvqPcIVAuiPGRFBSUAldz2A7F5V59jpRu5AqdflDqqX2ED9pnqb8yNAoVo8r9I-PeXFTlM8JHv85UncsF3WxFnEUXy3IWb_zIN48IsNfp3F3ibnBxb3KQ4rlcyY4vwvbcPwRxKD8EFYcT_ZwItNT_JTaSK--Wm6rM5GO2V-9zdeVD9vPj_sv8i7H7df99d3khoFi7StbmgAqluNY61bQrK9BeU61oQ179wAtSKqgZxDAuodo2PqO3aD09BcVB-2uscUf6-cFzP7TDydfhTXbLDvukZj3TZFerVJD3Zi48MYl2SpnIFnTzHw6Mv7davLFhvV9gXADaAUc048mmPycxnTIJiTIWYzxBRDzMkQ0xWm3phctOHAyTzGNYWygv9AL-YSjz8</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1855371243</pqid></control><display><type>article</type><title>Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill</title><source>Springer Link</source><creator>Saviak, M. P. ; Mel’nik, O. B. ; Uvarova, I. V. ; Kotko, A. V. ; Udovik, O. O.</creator><creatorcontrib>Saviak, M. P. ; Mel’nik, O. B. ; Uvarova, I. V. ; Kotko, A. V. ; Udovik, O. O.</creatorcontrib><description>Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zone. At the initial stage of grinding, texturing of titanium occurs and the titanium lattice cell increases in volume, thus inducing internal stresses. Based on these data, it is suggested that the introduction of carbon into the strained titanium particles leads to stacking faults in the titanium hcp lattice, acting as nuclei of fcc titanium carbide in the titanium sites fragmented. Single-crystal TiC 10–20 nm nanoparticles are formed in these sites. The length of titanium–carbon contacts naturally increases with grinding time, giving rise to more nuclei of the new fcc phase. This promotes a mechanically induced self-propagating reaction. The heat generated in the reaction contributes to the sintering of titanium carbide nanoparticles. This results in the formation of particle aggregates 0.1–0.5 μm in size.</description><identifier>ISSN: 1068-1302</identifier><identifier>EISSN: 1573-9066</identifier><identifier>DOI: 10.1007/s11106-016-9800-5</identifier><language>eng</language><publisher>New York: Springer US</publisher><subject>Carbides ; Carbon ; Ceramics ; Characterization and Evaluation of Materials ; Chemistry and Materials Science ; Composites ; Formations ; Glass ; Grinding ; Lattices ; Manufacturing Technology ; Materials Science ; Metallic Materials ; Mills ; Natural Materials ; Nuclei ; Powders ; Properties of Powders and Fibers ; Theory ; Titanium ; Titanium carbide</subject><ispartof>Powder metallurgy and metal ceramics, 2016-09, Vol.55 (5-6), p.251-258</ispartof><rights>Springer Science+Business Media New York 2016</rights><rights>COPYRIGHT 2016 Springer</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703</citedby><cites>FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Saviak, M. P.</creatorcontrib><creatorcontrib>Mel’nik, O. B.</creatorcontrib><creatorcontrib>Uvarova, I. V.</creatorcontrib><creatorcontrib>Kotko, A. V.</creatorcontrib><creatorcontrib>Udovik, O. O.</creatorcontrib><title>Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill</title><title>Powder metallurgy and metal ceramics</title><addtitle>Powder Metall Met Ceram</addtitle><description>Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zone. At the initial stage of grinding, texturing of titanium occurs and the titanium lattice cell increases in volume, thus inducing internal stresses. Based on these data, it is suggested that the introduction of carbon into the strained titanium particles leads to stacking faults in the titanium hcp lattice, acting as nuclei of fcc titanium carbide in the titanium sites fragmented. Single-crystal TiC 10–20 nm nanoparticles are formed in these sites. The length of titanium–carbon contacts naturally increases with grinding time, giving rise to more nuclei of the new fcc phase. This promotes a mechanically induced self-propagating reaction. The heat generated in the reaction contributes to the sintering of titanium carbide nanoparticles. This results in the formation of particle aggregates 0.1–0.5 μm in size.</description><subject>Carbides</subject><subject>Carbon</subject><subject>Ceramics</subject><subject>Characterization and Evaluation of Materials</subject><subject>Chemistry and Materials Science</subject><subject>Composites</subject><subject>Formations</subject><subject>Glass</subject><subject>Grinding</subject><subject>Lattices</subject><subject>Manufacturing Technology</subject><subject>Materials Science</subject><subject>Metallic Materials</subject><subject>Mills</subject><subject>Natural Materials</subject><subject>Nuclei</subject><subject>Powders</subject><subject>Properties of Powders and Fibers</subject><subject>Theory</subject><subject>Titanium</subject><subject>Titanium carbide</subject><issn>1068-1302</issn><issn>1573-9066</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2016</creationdate><recordtype>article</recordtype><recordid>eNp9kU1vFDEMhkeISpSWH8AtRy4p9nwks8eyogWpQA_lHCUez5JqJlmSmUP765tlkLihHBzF72PHfqvqPcIVAuiPGRFBSUAldz2A7F5V59jpRu5AqdflDqqX2ED9pnqb8yNAoVo8r9I-PeXFTlM8JHv85UncsF3WxFnEUXy3IWb_zIN48IsNfp3F3ibnBxb3KQ4rlcyY4vwvbcPwRxKD8EFYcT_ZwItNT_JTaSK--Wm6rM5GO2V-9zdeVD9vPj_sv8i7H7df99d3khoFi7StbmgAqluNY61bQrK9BeU61oQ179wAtSKqgZxDAuodo2PqO3aD09BcVB-2uscUf6-cFzP7TDydfhTXbLDvukZj3TZFerVJD3Zi48MYl2SpnIFnTzHw6Mv7davLFhvV9gXADaAUc048mmPycxnTIJiTIWYzxBRDzMkQ0xWm3phctOHAyTzGNYWygv9AL-YSjz8</recordid><startdate>20160901</startdate><enddate>20160901</enddate><creator>Saviak, M. P.</creator><creator>Mel’nik, O. B.</creator><creator>Uvarova, I. V.</creator><creator>Kotko, A. V.</creator><creator>Udovik, O. O.</creator><general>Springer US</general><general>Springer</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20160901</creationdate><title>Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill</title><author>Saviak, M. P. ; Mel’nik, O. B. ; Uvarova, I. V. ; Kotko, A. V. ; Udovik, O. O.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2016</creationdate><topic>Carbides</topic><topic>Carbon</topic><topic>Ceramics</topic><topic>Characterization and Evaluation of Materials</topic><topic>Chemistry and Materials Science</topic><topic>Composites</topic><topic>Formations</topic><topic>Glass</topic><topic>Grinding</topic><topic>Lattices</topic><topic>Manufacturing Technology</topic><topic>Materials Science</topic><topic>Metallic Materials</topic><topic>Mills</topic><topic>Natural Materials</topic><topic>Nuclei</topic><topic>Powders</topic><topic>Properties of Powders and Fibers</topic><topic>Theory</topic><topic>Titanium</topic><topic>Titanium carbide</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Saviak, M. P.</creatorcontrib><creatorcontrib>Mel’nik, O. B.</creatorcontrib><creatorcontrib>Uvarova, I. V.</creatorcontrib><creatorcontrib>Kotko, A. V.</creatorcontrib><creatorcontrib>Udovik, O. O.</creatorcontrib><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Powder metallurgy and metal ceramics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Saviak, M. P.</au><au>Mel’nik, O. B.</au><au>Uvarova, I. V.</au><au>Kotko, A. V.</au><au>Udovik, O. O.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill</atitle><jtitle>Powder metallurgy and metal ceramics</jtitle><stitle>Powder Metall Met Ceram</stitle><date>2016-09-01</date><risdate>2016</risdate><volume>55</volume><issue>5-6</issue><spage>251</spage><epage>258</epage><pages>251-258</pages><issn>1068-1302</issn><eissn>1573-9066</eissn><abstract>Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zone. At the initial stage of grinding, texturing of titanium occurs and the titanium lattice cell increases in volume, thus inducing internal stresses. Based on these data, it is suggested that the introduction of carbon into the strained titanium particles leads to stacking faults in the titanium hcp lattice, acting as nuclei of fcc titanium carbide in the titanium sites fragmented. Single-crystal TiC 10–20 nm nanoparticles are formed in these sites. The length of titanium–carbon contacts naturally increases with grinding time, giving rise to more nuclei of the new fcc phase. This promotes a mechanically induced self-propagating reaction. The heat generated in the reaction contributes to the sintering of titanium carbide nanoparticles. This results in the formation of particle aggregates 0.1–0.5 μm in size.</abstract><cop>New York</cop><pub>Springer US</pub><doi>10.1007/s11106-016-9800-5</doi><tpages>8</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1068-1302 |
ispartof | Powder metallurgy and metal ceramics, 2016-09, Vol.55 (5-6), p.251-258 |
issn | 1068-1302 1573-9066 |
language | eng |
recordid | cdi_proquest_miscellaneous_1855371243 |
source | Springer Link |
subjects | Carbides Carbon Ceramics Characterization and Evaluation of Materials Chemistry and Materials Science Composites Formations Glass Grinding Lattices Manufacturing Technology Materials Science Metallic Materials Mills Natural Materials Nuclei Powders Properties of Powders and Fibers Theory Titanium Titanium carbide |
title | Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T02%3A32%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-gale_proqu&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Crystallographic%20Features%20of%20Nanosized%20Titanium%20Carbide%20Produced%20from%20Titanium%20and%20Carbon%20in%20a%20Planetary-Ball%20Mill&rft.jtitle=Powder%20metallurgy%20and%20metal%20ceramics&rft.au=Saviak,%20M.%20P.&rft.date=2016-09-01&rft.volume=55&rft.issue=5-6&rft.spage=251&rft.epage=258&rft.pages=251-258&rft.issn=1068-1302&rft.eissn=1573-9066&rft_id=info:doi/10.1007/s11106-016-9800-5&rft_dat=%3Cgale_proqu%3EA470683648%3C/gale_proqu%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c360t-a473cd0c2471f274c1ca8a06b5e7c12e9bd026cc20cbb1c0c8be1bec85ebdb703%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=1855371243&rft_id=info:pmid/&rft_galeid=A470683648&rfr_iscdi=true |