Biochar properties and lead(II) adsorption capacity depend on feedstock type, pyrolysis temperature, and steam activation

Biochar is a promising material for facilitating the reclamation of oil sands process water (OSPW); however, how biochar properties can be optimized for metal removal from OSPW is not well studied. This study was conducted to determine relationships among feedstock type, pyrolysis condition, biochar...

Full description

Saved in:
Bibliographic Details
Published in:Chemosphere (Oxford) 2019-09, Vol.231, p.393-404
Main Authors: Kwak, Jin-Hyeob, Islam, Md Shahinoor, Wang, Siyuan, Messele, Selamawit Ashagre, Naeth, M. Anne, El-Din, Mohamed Gamal, Chang, Scott X.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Biochar is a promising material for facilitating the reclamation of oil sands process water (OSPW); however, how biochar properties can be optimized for metal removal from OSPW is not well studied. This study was conducted to determine relationships among feedstock type, pyrolysis condition, biochar property, and lead(II) adsorption capacity to demonstrate the potential use of biochar for metal removal from a synthetic OSPW. Sawdust, canola and wheat straw, and manure pellet were pyrolyzed at 300, 500, and 700 °C, with or without steam activation. Increasing pyrolysis temperature increased, with a few exceptions, biochar pH, surface area, and carbon content, but decreased hydrogen and oxygen contents and surface functional groups. Steam activation increased surface area but did not affect other properties. For non-steam-activated biochars, canola and wheat straw biochars produced at 700 °C had the highest lead(II) adsorption capacity (Qmax_Pb), at 108 and 109 mg g−1, respectively. Increasing the pyrolysis temperature increased Qmax_Pb due to increased biochar pH, ash content, and surface area by increasing precipitation, ion exchange, and inner-sphere complexation of lead(II). Steam activation increased lead(II) adsorption capacity for most biochars mainly due to the increased surface area, with the highest Qmax_Pb at 195 mg g−1 for canola straw biochar pyrolyzed at 700 °C with steam activation. The adsorption with time followed a pseudo-second order kinetic model. The results of this study will help select most effective biochars that can be produced from locally available agricultural or forestry byproducts that are optimized for metal removal from synthetic OSPW. •Relationships among feedstock type, pyrolysis conditions, biochar properties, and Qmax of lead(II) (Qmax_Pb) were tested•Biochar properties and Qmax_Pb depended on feedstock type, pyrolysis temperature, and steam activation•Canola straw biochar had highest and sawdust biochar had lowest Qmax_Pb•Increases in pyrolysis temperature and steam activation increased Qmax_Pb•Lead(II) adsorption followed the pseudo-second order kinetic model
ISSN:0045-6535
1879-1298
DOI:10.1016/j.chemosphere.2019.05.128