Accelerated weathering affects the chemical and physical properties of marine antifouling paint microplastics and their identification by ATR-FTIR spectroscopy

Microplastics prepared from commercial marine antifouling paints were weathered by UV-C irradiation representing between 25 and 101 days of real-time, outdoor exposure. Attenuated Total Reflection Fourier Transform Infrared (ATR-FTIR) spectroscopy of the degraded paint particles showed that weatheri...

Full description

Saved in:
Bibliographic Details
Published in:Chemosphere (Oxford) 2021-07, Vol.274, p.129749-129749, Article 129749
Main Authors: Simon, Márta, Vianello, Alvise, Shashoua, Yvonne, Vollertsen, Jes
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Microplastics prepared from commercial marine antifouling paints were weathered by UV-C irradiation representing between 25 and 101 days of real-time, outdoor exposure. Attenuated Total Reflection Fourier Transform Infrared (ATR-FTIR) spectroscopy of the degraded paint particles showed that weathering induced chemical changes in the material, including the release of volatile components and the formation of hydrophilic groups. The chemical changes and increased reactivity of the paint binder were associated with alterations in their physical properties and increased leaching of metals in freshwater conditions. Changes in the spectra obtained from weathered paint samples reduced their match with spectra of unaged materials, resulting in a poorer similarity index, the Score when using automatic identification tools for microplastics. The results suggest that spectra of weathered, as well as pristine paint microplastics, should be consulted when applying analytical pipelines to identify microplastics extracted from natural matrices. [Display omitted] •Weathering impairs the binder structure of antifouling paint microparticles.•Impaired binder structure leads to increased heavy metal release.•Weathering hinders the identification of paints based on their infrared spectra.
ISSN:0045-6535
1879-1298
DOI:10.1016/j.chemosphere.2021.129749