Preparation of Poly (oxytetramethylene) -Aramid Block Copolymers by the Direct Polycondensation Method
Poly (oxytetramethylene) -aramid block copolymers 5 having inherent viscosities of 0.2-0.5dl/g were prepared by the direct polycondensation reaction using triphenyl phosphite and pyridine as condensing reagents from amine-terminated poly (oxytetramethylene) 4 and carboxyl-terminated aromatic polyami...
Saved in:
Published in: | KOBUNSHI RONBUNSHU 1988/02/25, Vol.45(2), pp.185-188 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | eng ; jpn |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Poly (oxytetramethylene) -aramid block copolymers 5 having inherent viscosities of 0.2-0.5dl/g were prepared by the direct polycondensation reaction using triphenyl phosphite and pyridine as condensing reagents from amine-terminated poly (oxytetramethylene) 4 and carboxyl-terminated aromatic polyamides (aramids) 3, which were prepared directly from 3, 4′-oxydianiline and a calculated excess of isophthalic acid. Block copolymers 5 were soluble in amide type solvents that were good solvents for aramids. Thermogravimetry curves of the polymers indicated that 5 decomposed in two steps, and the decomposition curves were between, those of 3 and 4. |
---|---|
ISSN: | 0386-2186 1881-5685 |
DOI: | 10.1295/koron.45.185 |