Loading…
Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method
The superconducting powders in the Bi--Pb--Sr--Ca--Cu--O system were easily prepared from water in oil type emulsion by loading the bismuth, Pb, Sr, Ca and Cu ions into the aqueous phase. The low T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 1 Cu sub 2 O sub y ) was formed by calcining at 800 deg C fo...
Saved in:
Published in: | Solid state communications 1990-08, Vol.75 (5), p.455-458 |
---|---|
Main Authors: | , |
Format: | Article |
Language: | English |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | |
---|---|
cites | |
container_end_page | 458 |
container_issue | 5 |
container_start_page | 455 |
container_title | Solid state communications |
container_volume | 75 |
creator | Um, W S Kim, H G |
description | The superconducting powders in the Bi--Pb--Sr--Ca--Cu--O system were easily prepared from water in oil type emulsion by loading the bismuth, Pb, Sr, Ca and Cu ions into the aqueous phase. The low T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 1 Cu sub 2 O sub y ) was formed by calcining at 800 deg C for 10 h in a low oxygen partial pressure of 1/20 atm. The shape of the calcined powder is thin plate of size approx 2 mu m and thickness < 0.5 mu m. It was observed that the high T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 2 Cu sub 3 O sub y ) was formed by sintering at 850 deg C for 30 h in O pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a T sub c (zero) = 105K. 12 ref.--AA |
format | article |
fullrecord | <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_miscellaneous_24974096</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>24974096</sourcerecordid><originalsourceid>FETCH-proquest_miscellaneous_249740963</originalsourceid><addsrcrecordid>eNqNjbkKwkAURadQcP2HV9k9GBdM0rphIwaXWibmaUaSTJw3g6Tx213wAywupzgHbkO0pRyHOJRR2BId5puUMgiDYVs8d6rSKayMLZTTpgRzAZcRrPU1gwOwT-AMcaaYQJdfM9OIcYK4t4hz9Z5H3MK-ZkcFHFmXV4jNIyXLEFuqlKUUkhqWhc_5c7Cw9afZkMtM2hPNi8qZ-j92xWC1PMzXWFlz98TuVGg-U56rkozn02gSBRMZTcd_hy9VgE7Y</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>24974096</pqid></control><display><type>article</type><title>Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method</title><source>Elsevier SD Backfile Physics</source><source>Backfile Package - Materials Science [YMS]</source><creator>Um, W S ; Kim, H G</creator><creatorcontrib>Um, W S ; Kim, H G</creatorcontrib><description>The superconducting powders in the Bi--Pb--Sr--Ca--Cu--O system were easily prepared from water in oil type emulsion by loading the bismuth, Pb, Sr, Ca and Cu ions into the aqueous phase. The low T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 1 Cu sub 2 O sub y ) was formed by calcining at 800 deg C for 10 h in a low oxygen partial pressure of 1/20 atm. The shape of the calcined powder is thin plate of size approx 2 mu m and thickness < 0.5 mu m. It was observed that the high T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 2 Cu sub 3 O sub y ) was formed by sintering at 850 deg C for 30 h in O pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a T sub c (zero) = 105K. 12 ref.--AA</description><identifier>ISSN: 0038-1098</identifier><language>eng</language><ispartof>Solid state communications, 1990-08, Vol.75 (5), p.455-458</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784</link.rule.ids></links><search><creatorcontrib>Um, W S</creatorcontrib><creatorcontrib>Kim, H G</creatorcontrib><title>Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method</title><title>Solid state communications</title><description>The superconducting powders in the Bi--Pb--Sr--Ca--Cu--O system were easily prepared from water in oil type emulsion by loading the bismuth, Pb, Sr, Ca and Cu ions into the aqueous phase. The low T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 1 Cu sub 2 O sub y ) was formed by calcining at 800 deg C for 10 h in a low oxygen partial pressure of 1/20 atm. The shape of the calcined powder is thin plate of size approx 2 mu m and thickness < 0.5 mu m. It was observed that the high T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 2 Cu sub 3 O sub y ) was formed by sintering at 850 deg C for 30 h in O pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a T sub c (zero) = 105K. 12 ref.--AA</description><issn>0038-1098</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1990</creationdate><recordtype>article</recordtype><recordid>eNqNjbkKwkAURadQcP2HV9k9GBdM0rphIwaXWibmaUaSTJw3g6Tx213wAywupzgHbkO0pRyHOJRR2BId5puUMgiDYVs8d6rSKayMLZTTpgRzAZcRrPU1gwOwT-AMcaaYQJdfM9OIcYK4t4hz9Z5H3MK-ZkcFHFmXV4jNIyXLEFuqlKUUkhqWhc_5c7Cw9afZkMtM2hPNi8qZ-j92xWC1PMzXWFlz98TuVGg-U56rkozn02gSBRMZTcd_hy9VgE7Y</recordid><startdate>19900801</startdate><enddate>19900801</enddate><creator>Um, W S</creator><creator>Kim, H G</creator><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>19900801</creationdate><title>Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method</title><author>Um, W S ; Kim, H G</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-proquest_miscellaneous_249740963</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1990</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Um, W S</creatorcontrib><creatorcontrib>Kim, H G</creatorcontrib><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Solid state communications</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Um, W S</au><au>Kim, H G</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method</atitle><jtitle>Solid state communications</jtitle><date>1990-08-01</date><risdate>1990</risdate><volume>75</volume><issue>5</issue><spage>455</spage><epage>458</epage><pages>455-458</pages><issn>0038-1098</issn><abstract>The superconducting powders in the Bi--Pb--Sr--Ca--Cu--O system were easily prepared from water in oil type emulsion by loading the bismuth, Pb, Sr, Ca and Cu ions into the aqueous phase. The low T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 1 Cu sub 2 O sub y ) was formed by calcining at 800 deg C for 10 h in a low oxygen partial pressure of 1/20 atm. The shape of the calcined powder is thin plate of size approx 2 mu m and thickness < 0.5 mu m. It was observed that the high T sub c phase (Bi(Pb) sub 2 Sr sub 2 Ca sub 2 Cu sub 3 O sub y ) was formed by sintering at 850 deg C for 30 h in O pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a T sub c (zero) = 105K. 12 ref.--AA</abstract></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0038-1098 |
ispartof | Solid state communications, 1990-08, Vol.75 (5), p.455-458 |
issn | 0038-1098 |
language | eng |
recordid | cdi_proquest_miscellaneous_24974096 |
source | Elsevier SD Backfile Physics; Backfile Package - Materials Science [YMS] |
title | Rapid Formation of the High T sub c Phase in the Bi--Pb--Sr--Ca--Cu--O System Using Powders Prepared by Emulsion Drying Method |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T14%3A45%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Rapid%20Formation%20of%20the%20High%20T%20sub%20c%20Phase%20in%20the%20Bi--Pb--Sr--Ca--Cu--O%20System%20Using%20Powders%20Prepared%20by%20Emulsion%20Drying%20Method&rft.jtitle=Solid%20state%20communications&rft.au=Um,%20W%20S&rft.date=1990-08-01&rft.volume=75&rft.issue=5&rft.spage=455&rft.epage=458&rft.pages=455-458&rft.issn=0038-1098&rft_id=info:doi/&rft_dat=%3Cproquest%3E24974096%3C/proquest%3E%3Cgrp_id%3Ecdi_FETCH-proquest_miscellaneous_249740963%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=24974096&rft_id=info:pmid/&rfr_iscdi=true |