Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography

This paper describes the experimental work conducted on creep and fatigue crack growth behaviour in axially-notched, seam-welded pipes. The key objective of this work is to examine how the results from feature tests compare with standard laboratory specimen data using different European high tempera...

Full description

Saved in:
Bibliographic Details
Published in:International journal of pressure vessels and piping 2001-11, Vol.78 (11), p.819-826
Main Authors: Le Mat Hamata, N, Shibli, I.A
Format: Article
Language:English
Subjects:
Citations: Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c368t-dc4ab0968b8d5b478fc27178a3b7ab57177bf82199b42681294c5cc8bac89fab3
cites
container_end_page 826
container_issue 11
container_start_page 819
container_title International journal of pressure vessels and piping
container_volume 78
creator Le Mat Hamata, N
Shibli, I.A
description This paper describes the experimental work conducted on creep and fatigue crack growth behaviour in axially-notched, seam-welded pipes. The key objective of this work is to examine how the results from feature tests compare with standard laboratory specimen data using different European high temperature assessment methods, the final aim being to contribute towards the development and validation of a unified European procedure for estimating crack growth behaviour and remaining life of high temperature components. Within the context of this work, two steels P22 (2 1/4Cr1Mo) and P91 (9Cr1MoVNb) were studied at 565 and 625 °C, respectively. Two pipes were tested for each material; one pipe was subjected to a constant gas pressure (SP) and the other was tested under low cyclic pressure (CP) (10 −4 Hz). Each pipe contained three axially machined notches, one in the heat affected zone (HAZ) and two in the base metal. The direct current (DC) potential drop (PD) technique was successfully applied to monitor crack growth during the tests. In both steels, the defect situated in the HAZ exhibited a higher crack growth rate, confirming that the HAZ is more vulnerable to crack initiation and propagation than the parent metal. Post-test metallography analysis showed that creep cavitation damage is the main mechanism governing the crack propagation. In the case of the cyclic tests for which the selected frequency was close to, or slightly higher than, the frequencies encountered in high temperature plants, metallographic observations showed no noticeable effect of cyclic loading in terms of transgranular crack growth. The data analysis of the experimental data obtained in this work are presented in Part II of this paper [Creep Crack Growth of Seam-welded P22 and P91 Pipes with Artificial defects—Part II. Data analysis. Second International HIDA Conference, Advances in Defects Assessment in High Temperature Plant, MPA, Stuttgart, Germany, 4–6 October, 2000].
doi_str_mv 10.1016/S0308-0161(01)00096-5
format article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_26680350</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0308016101000965</els_id><sourcerecordid>26680350</sourcerecordid><originalsourceid>FETCH-LOGICAL-c368t-dc4ab0968b8d5b478fc27178a3b7ab57177bf82199b42681294c5cc8bac89fab3</originalsourceid><addsrcrecordid>eNqFUMFu1DAQtSqQuhQ-AckXEByy2EmcOCeEVi2tVIlKwNkaT8at22wSbC_LnvvjeHercuQyM5p582beY-ytFEspZPPpu6iELnIlPwj5UQjRNYU6YQup266oVC1fsMUz5JS9ivFeCNkK1SzY4yoQzRwD4AO_DdM23fHJ8UiwLrY09NTzm7LkMObcST77mSLf-oyCkLzz6GHgPTnCFJf8Jjf51ZKf_5kp-DWNKU9j2vS7A8M8xVQkiomvKU-G6TbAfLd7zV46GCK9ecpn7OfF-Y_VZXH97evV6st1gVWjU9FjDTZr01b3ytatdli2stVQ2RasymVrnS5l19m6bLQsuxoVoraAunNgqzP2_sg7h-nXJr9h1j4iDQOMNG2iKZtGi0qJDFRHIIYpxkDOzFkNhJ2RwuwtNwfLzd7PHMzBcqPy3runAxARBhdgRB__LVd1pyqx5_98xFFW-9tTMBE9jUi9D9lI00_-P5f-Aua7le8</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>26680350</pqid></control><display><type>article</type><title>Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography</title><source>Elsevier:Jisc Collections:Elsevier Read and Publish Agreement 2022-2024:Freedom Collection (Reading list)</source><creator>Le Mat Hamata, N ; Shibli, I.A</creator><creatorcontrib>Le Mat Hamata, N ; Shibli, I.A</creatorcontrib><description>This paper describes the experimental work conducted on creep and fatigue crack growth behaviour in axially-notched, seam-welded pipes. The key objective of this work is to examine how the results from feature tests compare with standard laboratory specimen data using different European high temperature assessment methods, the final aim being to contribute towards the development and validation of a unified European procedure for estimating crack growth behaviour and remaining life of high temperature components. Within the context of this work, two steels P22 (2 1/4Cr1Mo) and P91 (9Cr1MoVNb) were studied at 565 and 625 °C, respectively. Two pipes were tested for each material; one pipe was subjected to a constant gas pressure (SP) and the other was tested under low cyclic pressure (CP) (10 −4 Hz). Each pipe contained three axially machined notches, one in the heat affected zone (HAZ) and two in the base metal. The direct current (DC) potential drop (PD) technique was successfully applied to monitor crack growth during the tests. In both steels, the defect situated in the HAZ exhibited a higher crack growth rate, confirming that the HAZ is more vulnerable to crack initiation and propagation than the parent metal. Post-test metallography analysis showed that creep cavitation damage is the main mechanism governing the crack propagation. In the case of the cyclic tests for which the selected frequency was close to, or slightly higher than, the frequencies encountered in high temperature plants, metallographic observations showed no noticeable effect of cyclic loading in terms of transgranular crack growth. The data analysis of the experimental data obtained in this work are presented in Part II of this paper [Creep Crack Growth of Seam-welded P22 and P91 Pipes with Artificial defects—Part II. Data analysis. Second International HIDA Conference, Advances in Defects Assessment in High Temperature Plant, MPA, Stuttgart, Germany, 4–6 October, 2000].</description><identifier>ISSN: 0308-0161</identifier><identifier>EISSN: 1879-3541</identifier><identifier>DOI: 10.1016/S0308-0161(01)00096-5</identifier><identifier>CODEN: PRVPAS</identifier><language>eng</language><publisher>Oxford: Elsevier Ltd</publisher><subject>Applied sciences ; Cavitations ; Creep and fatigue crack growth ; Exact sciences and technology ; Fractures ; Mechanical engineering. Machine design ; Mechanical properties and methods of testing. Rheology. Fracture mechanics. Tribology ; Metals. Metallurgy ; P22 ; P91 ; Seam-welded pipe ; Steel design ; Steel tanks and pressure vessels; boiler manufacturing</subject><ispartof>International journal of pressure vessels and piping, 2001-11, Vol.78 (11), p.819-826</ispartof><rights>2002</rights><rights>2002 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c368t-dc4ab0968b8d5b478fc27178a3b7ab57177bf82199b42681294c5cc8bac89fab3</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>309,310,314,780,784,789,790,23928,23929,25138,27922,27923</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=13495300$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Le Mat Hamata, N</creatorcontrib><creatorcontrib>Shibli, I.A</creatorcontrib><title>Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography</title><title>International journal of pressure vessels and piping</title><description>This paper describes the experimental work conducted on creep and fatigue crack growth behaviour in axially-notched, seam-welded pipes. The key objective of this work is to examine how the results from feature tests compare with standard laboratory specimen data using different European high temperature assessment methods, the final aim being to contribute towards the development and validation of a unified European procedure for estimating crack growth behaviour and remaining life of high temperature components. Within the context of this work, two steels P22 (2 1/4Cr1Mo) and P91 (9Cr1MoVNb) were studied at 565 and 625 °C, respectively. Two pipes were tested for each material; one pipe was subjected to a constant gas pressure (SP) and the other was tested under low cyclic pressure (CP) (10 −4 Hz). Each pipe contained three axially machined notches, one in the heat affected zone (HAZ) and two in the base metal. The direct current (DC) potential drop (PD) technique was successfully applied to monitor crack growth during the tests. In both steels, the defect situated in the HAZ exhibited a higher crack growth rate, confirming that the HAZ is more vulnerable to crack initiation and propagation than the parent metal. Post-test metallography analysis showed that creep cavitation damage is the main mechanism governing the crack propagation. In the case of the cyclic tests for which the selected frequency was close to, or slightly higher than, the frequencies encountered in high temperature plants, metallographic observations showed no noticeable effect of cyclic loading in terms of transgranular crack growth. The data analysis of the experimental data obtained in this work are presented in Part II of this paper [Creep Crack Growth of Seam-welded P22 and P91 Pipes with Artificial defects—Part II. Data analysis. Second International HIDA Conference, Advances in Defects Assessment in High Temperature Plant, MPA, Stuttgart, Germany, 4–6 October, 2000].</description><subject>Applied sciences</subject><subject>Cavitations</subject><subject>Creep and fatigue crack growth</subject><subject>Exact sciences and technology</subject><subject>Fractures</subject><subject>Mechanical engineering. Machine design</subject><subject>Mechanical properties and methods of testing. Rheology. Fracture mechanics. Tribology</subject><subject>Metals. Metallurgy</subject><subject>P22</subject><subject>P91</subject><subject>Seam-welded pipe</subject><subject>Steel design</subject><subject>Steel tanks and pressure vessels; boiler manufacturing</subject><issn>0308-0161</issn><issn>1879-3541</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2001</creationdate><recordtype>article</recordtype><recordid>eNqFUMFu1DAQtSqQuhQ-AckXEByy2EmcOCeEVi2tVIlKwNkaT8at22wSbC_LnvvjeHercuQyM5p582beY-ytFEspZPPpu6iELnIlPwj5UQjRNYU6YQup266oVC1fsMUz5JS9ivFeCNkK1SzY4yoQzRwD4AO_DdM23fHJ8UiwLrY09NTzm7LkMObcST77mSLf-oyCkLzz6GHgPTnCFJf8Jjf51ZKf_5kp-DWNKU9j2vS7A8M8xVQkiomvKU-G6TbAfLd7zV46GCK9ecpn7OfF-Y_VZXH97evV6st1gVWjU9FjDTZr01b3ytatdli2stVQ2RasymVrnS5l19m6bLQsuxoVoraAunNgqzP2_sg7h-nXJr9h1j4iDQOMNG2iKZtGi0qJDFRHIIYpxkDOzFkNhJ2RwuwtNwfLzd7PHMzBcqPy3runAxARBhdgRB__LVd1pyqx5_98xFFW-9tTMBE9jUi9D9lI00_-P5f-Aua7le8</recordid><startdate>20011101</startdate><enddate>20011101</enddate><creator>Le Mat Hamata, N</creator><creator>Shibli, I.A</creator><general>Elsevier Ltd</general><general>Elsevier</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7TB</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>KR7</scope></search><sort><creationdate>20011101</creationdate><title>Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography</title><author>Le Mat Hamata, N ; Shibli, I.A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c368t-dc4ab0968b8d5b478fc27178a3b7ab57177bf82199b42681294c5cc8bac89fab3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2001</creationdate><topic>Applied sciences</topic><topic>Cavitations</topic><topic>Creep and fatigue crack growth</topic><topic>Exact sciences and technology</topic><topic>Fractures</topic><topic>Mechanical engineering. Machine design</topic><topic>Mechanical properties and methods of testing. Rheology. Fracture mechanics. Tribology</topic><topic>Metals. Metallurgy</topic><topic>P22</topic><topic>P91</topic><topic>Seam-welded pipe</topic><topic>Steel design</topic><topic>Steel tanks and pressure vessels; boiler manufacturing</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Le Mat Hamata, N</creatorcontrib><creatorcontrib>Shibli, I.A</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Mechanical &amp; Transportation Engineering Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>International journal of pressure vessels and piping</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Le Mat Hamata, N</au><au>Shibli, I.A</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography</atitle><jtitle>International journal of pressure vessels and piping</jtitle><date>2001-11-01</date><risdate>2001</risdate><volume>78</volume><issue>11</issue><spage>819</spage><epage>826</epage><pages>819-826</pages><issn>0308-0161</issn><eissn>1879-3541</eissn><coden>PRVPAS</coden><abstract>This paper describes the experimental work conducted on creep and fatigue crack growth behaviour in axially-notched, seam-welded pipes. The key objective of this work is to examine how the results from feature tests compare with standard laboratory specimen data using different European high temperature assessment methods, the final aim being to contribute towards the development and validation of a unified European procedure for estimating crack growth behaviour and remaining life of high temperature components. Within the context of this work, two steels P22 (2 1/4Cr1Mo) and P91 (9Cr1MoVNb) were studied at 565 and 625 °C, respectively. Two pipes were tested for each material; one pipe was subjected to a constant gas pressure (SP) and the other was tested under low cyclic pressure (CP) (10 −4 Hz). Each pipe contained three axially machined notches, one in the heat affected zone (HAZ) and two in the base metal. The direct current (DC) potential drop (PD) technique was successfully applied to monitor crack growth during the tests. In both steels, the defect situated in the HAZ exhibited a higher crack growth rate, confirming that the HAZ is more vulnerable to crack initiation and propagation than the parent metal. Post-test metallography analysis showed that creep cavitation damage is the main mechanism governing the crack propagation. In the case of the cyclic tests for which the selected frequency was close to, or slightly higher than, the frequencies encountered in high temperature plants, metallographic observations showed no noticeable effect of cyclic loading in terms of transgranular crack growth. The data analysis of the experimental data obtained in this work are presented in Part II of this paper [Creep Crack Growth of Seam-welded P22 and P91 Pipes with Artificial defects—Part II. Data analysis. Second International HIDA Conference, Advances in Defects Assessment in High Temperature Plant, MPA, Stuttgart, Germany, 4–6 October, 2000].</abstract><cop>Oxford</cop><pub>Elsevier Ltd</pub><doi>10.1016/S0308-0161(01)00096-5</doi><tpages>8</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0308-0161
ispartof International journal of pressure vessels and piping, 2001-11, Vol.78 (11), p.819-826
issn 0308-0161
1879-3541
language eng
recordid cdi_proquest_miscellaneous_26680350
source Elsevier:Jisc Collections:Elsevier Read and Publish Agreement 2022-2024:Freedom Collection (Reading list)
subjects Applied sciences
Cavitations
Creep and fatigue crack growth
Exact sciences and technology
Fractures
Mechanical engineering. Machine design
Mechanical properties and methods of testing. Rheology. Fracture mechanics. Tribology
Metals. Metallurgy
P22
P91
Seam-welded pipe
Steel design
Steel tanks and pressure vessels
boiler manufacturing
title Creep crack growth of seam-welded P22 and P91 pipes with artificial defects. Part I. Experimental study and post-test metallography
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T12%3A29%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Creep%20crack%20growth%20of%20seam-welded%20P22%20and%20P91%20pipes%20with%20artificial%20defects.%20Part%20I.%20Experimental%20study%20and%20post-test%20metallography&rft.jtitle=International%20journal%20of%20pressure%20vessels%20and%20piping&rft.au=Le%20Mat%20Hamata,%20N&rft.date=2001-11-01&rft.volume=78&rft.issue=11&rft.spage=819&rft.epage=826&rft.pages=819-826&rft.issn=0308-0161&rft.eissn=1879-3541&rft.coden=PRVPAS&rft_id=info:doi/10.1016/S0308-0161(01)00096-5&rft_dat=%3Cproquest_cross%3E26680350%3C/proquest_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c368t-dc4ab0968b8d5b478fc27178a3b7ab57177bf82199b42681294c5cc8bac89fab3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=26680350&rft_id=info:pmid/&rfr_iscdi=true