Loading…

Electrochemical and crystallographic characterization of Co-free hydrogen storage alloys for use in nickel–metal hydride batteries

Electrochemical and crystallographic characterization of Co-free hydrogen storage alloys containing Si and/or Fe was carried out. In the charge–discharge cycle test, the maximum discharge capacity of a Co-free MmNi 4.3Mn 0.4Al 0.3 (Mm=misch metal) alloy electrode was decreased by the partial substit...

Full description

Saved in:
Bibliographic Details
Published in:Electrochimica acta 2001-08, Vol.46 (28), p.4383-4388
Main Authors: Iwakura, Chiaki, Ohkawa, Kazuhiro, Senoh, Hiroshi, Inoue, Hiroshi
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Electrochemical and crystallographic characterization of Co-free hydrogen storage alloys containing Si and/or Fe was carried out. In the charge–discharge cycle test, the maximum discharge capacity of a Co-free MmNi 4.3Mn 0.4Al 0.3 (Mm=misch metal) alloy electrode was decreased by the partial substitution of Si and/or Fe for Ni, but the cycle performance was improved. The MmNi 3.6Mn 0.4Al 0.3Si 0.1Fe 0.6 electrode showed the most excellent cycle durability in this study. It was found by SEM, EPMA and XRD that Fe and Si contained in these alloys more or less suppressed the dissolution of Al and the lattice expansion with hydrogen absorption, leading to the long cycle life. This effect was strengthened by the simultaneous partial substitution of Si and Fe for Ni in the Co-free alloy.
ISSN:0013-4686
1873-3859
DOI:10.1016/S0013-4686(01)00724-1