Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites

A study was conducted to evaluate the use of elevated pressure to accelerate the rate of thermo-oxidative degradation in polymeric composite materials. The motivation for this work was based on earlier studies by Tsotsis [1, 2], Kerr and Haskins [3]and by Ciutacu, et al. [4]which demonstrated that h...

Full description

Saved in:
Bibliographic Details
Published in:Polymer degradation and stability 1999-01, Vol.64 (2), p.207-212
Main Authors: Tsotsis, Thomas K., Keller, Scott, Bardis, Jason, Bish, Jack
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533
cites cdi_FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533
container_end_page 212
container_issue 2
container_start_page 207
container_title Polymer degradation and stability
container_volume 64
creator Tsotsis, Thomas K.
Keller, Scott
Bardis, Jason
Bish, Jack
description A study was conducted to evaluate the use of elevated pressure to accelerate the rate of thermo-oxidative degradation in polymeric composite materials. The motivation for this work was based on earlier studies by Tsotsis [1, 2], Kerr and Haskins [3]and by Ciutacu, et al. [4]which demonstrated that higher pressures of air or oxygen tended to increase the rate of degradation of polymeric composites. Moreover, accelerated aging methods are needed to evaluate materials which are to be used under long-term exposure to elevated temperature in oxidative environments such as the High-Speed Civil Transport (HSCT). The methodology proposed herein augments elevated temperature aging with elevated pressure to accelerate the rate of thermo-oxidative degradation. Temperatures below those used by previous workers were employed in order to avoid anomalous non-linear effects which can occur near the glass-transition temperature of polymeric materials. In the present work, Hexcel AS4/3501-6 [±45°] 2 s shear and [+45°/0°/−45°/90°] 2 s quasi-isotropic Hexcel IM7/8552 open hole compression specimens were aged at 121°C (250°F) at pressures of 0.101, 0.345, 1.03, and 1.72 MPa (14.7, 50, 150, and 250 psi). Three pressure vessels were designed and built to contain the prescribed pressures. These vessels were placed inside an oven and used an air bleed to recycle the air inside the vessels. For the open hole testing, a test method was derived from Boeing BSS 7260 to reduce the material required for each specimen. Specimens were tested as-made and after 1000 h exposure to each of the pressures. Results show up to a 20% reduction in tensile shear strength for the [±45°] 2 s specimens but show no decrease in open hole compression strength though weight losses and visible discoloration of the specimens are present in both materials. Differences are attributed to the different lay-ups used as well as the different materials systems of the two specimen types.
doi_str_mv 10.1016/S0141-3910(98)00190-6
format article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_27089029</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0141391098001906</els_id><sourcerecordid>27089029</sourcerecordid><originalsourceid>FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533</originalsourceid><addsrcrecordid>eNqFkEFr3DAQhUVIIZttf0JBh1LSg5ORtbKsUwlL2gQWEmhyFrI03qrY1layl_TfV94NyTG6jJj5nt7oEfKZwSUDVl39ArZiBVcMLlT9DYApKKoTsmC15EXJS3ZKFq_IGTlP6Q_ksxJsQfxDxM73fjDxH8W96SYz-jDQ0NLxN9Ip4XzFLo9GdHQXMaUpIh0DNdbmfsz9GY19KMKzd1m-R2q2fthSP1Ab-l1IfsT0kXxoTZfw00tdkqcfN4_r22Jz__Nufb0pLK_kWKA1rnWApuEgpawaaFBUjXC1KkvJmlpwdCvM5uWqrZUCEAJcUzPBrZSC8yX5enx3F8PfCdOoe5_ypp0ZMExJlxJqBaXKoDiCNoaUIrZ6F32fc9AM9BysPgSr59S0qvUhWF1l3ZcXA5Os6dpoBuvTmzgvWkmWse9HDPNn9x6jTtbjYNH5iHbULvh3jP4DxTqOgg</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>27089029</pqid></control><display><type>article</type><title>Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites</title><source>Elsevier</source><creator>Tsotsis, Thomas K. ; Keller, Scott ; Bardis, Jason ; Bish, Jack</creator><creatorcontrib>Tsotsis, Thomas K. ; Keller, Scott ; Bardis, Jason ; Bish, Jack</creatorcontrib><description>A study was conducted to evaluate the use of elevated pressure to accelerate the rate of thermo-oxidative degradation in polymeric composite materials. The motivation for this work was based on earlier studies by Tsotsis [1, 2], Kerr and Haskins [3]and by Ciutacu, et al. [4]which demonstrated that higher pressures of air or oxygen tended to increase the rate of degradation of polymeric composites. Moreover, accelerated aging methods are needed to evaluate materials which are to be used under long-term exposure to elevated temperature in oxidative environments such as the High-Speed Civil Transport (HSCT). The methodology proposed herein augments elevated temperature aging with elevated pressure to accelerate the rate of thermo-oxidative degradation. Temperatures below those used by previous workers were employed in order to avoid anomalous non-linear effects which can occur near the glass-transition temperature of polymeric materials. In the present work, Hexcel AS4/3501-6 [±45°] 2 s shear and [+45°/0°/−45°/90°] 2 s quasi-isotropic Hexcel IM7/8552 open hole compression specimens were aged at 121°C (250°F) at pressures of 0.101, 0.345, 1.03, and 1.72 MPa (14.7, 50, 150, and 250 psi). Three pressure vessels were designed and built to contain the prescribed pressures. These vessels were placed inside an oven and used an air bleed to recycle the air inside the vessels. For the open hole testing, a test method was derived from Boeing BSS 7260 to reduce the material required for each specimen. Specimens were tested as-made and after 1000 h exposure to each of the pressures. Results show up to a 20% reduction in tensile shear strength for the [±45°] 2 s specimens but show no decrease in open hole compression strength though weight losses and visible discoloration of the specimens are present in both materials. Differences are attributed to the different lay-ups used as well as the different materials systems of the two specimen types.</description><identifier>ISSN: 0141-3910</identifier><identifier>EISSN: 1873-2321</identifier><identifier>DOI: 10.1016/S0141-3910(98)00190-6</identifier><identifier>CODEN: PDSTDW</identifier><language>eng</language><publisher>Oxford: Elsevier Ltd</publisher><subject>Applied sciences ; Exact sciences and technology ; Forms of application and semi-finished materials ; Laminates ; Polymer industry, paints, wood ; Technology of polymers</subject><ispartof>Polymer degradation and stability, 1999-01, Vol.64 (2), p.207-212</ispartof><rights>1999 Elsevier Science Ltd</rights><rights>1999 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533</citedby><cites>FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27915,27916</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=1892671$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Tsotsis, Thomas K.</creatorcontrib><creatorcontrib>Keller, Scott</creatorcontrib><creatorcontrib>Bardis, Jason</creatorcontrib><creatorcontrib>Bish, Jack</creatorcontrib><title>Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites</title><title>Polymer degradation and stability</title><description>A study was conducted to evaluate the use of elevated pressure to accelerate the rate of thermo-oxidative degradation in polymeric composite materials. The motivation for this work was based on earlier studies by Tsotsis [1, 2], Kerr and Haskins [3]and by Ciutacu, et al. [4]which demonstrated that higher pressures of air or oxygen tended to increase the rate of degradation of polymeric composites. Moreover, accelerated aging methods are needed to evaluate materials which are to be used under long-term exposure to elevated temperature in oxidative environments such as the High-Speed Civil Transport (HSCT). The methodology proposed herein augments elevated temperature aging with elevated pressure to accelerate the rate of thermo-oxidative degradation. Temperatures below those used by previous workers were employed in order to avoid anomalous non-linear effects which can occur near the glass-transition temperature of polymeric materials. In the present work, Hexcel AS4/3501-6 [±45°] 2 s shear and [+45°/0°/−45°/90°] 2 s quasi-isotropic Hexcel IM7/8552 open hole compression specimens were aged at 121°C (250°F) at pressures of 0.101, 0.345, 1.03, and 1.72 MPa (14.7, 50, 150, and 250 psi). Three pressure vessels were designed and built to contain the prescribed pressures. These vessels were placed inside an oven and used an air bleed to recycle the air inside the vessels. For the open hole testing, a test method was derived from Boeing BSS 7260 to reduce the material required for each specimen. Specimens were tested as-made and after 1000 h exposure to each of the pressures. Results show up to a 20% reduction in tensile shear strength for the [±45°] 2 s specimens but show no decrease in open hole compression strength though weight losses and visible discoloration of the specimens are present in both materials. Differences are attributed to the different lay-ups used as well as the different materials systems of the two specimen types.</description><subject>Applied sciences</subject><subject>Exact sciences and technology</subject><subject>Forms of application and semi-finished materials</subject><subject>Laminates</subject><subject>Polymer industry, paints, wood</subject><subject>Technology of polymers</subject><issn>0141-3910</issn><issn>1873-2321</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1999</creationdate><recordtype>article</recordtype><recordid>eNqFkEFr3DAQhUVIIZttf0JBh1LSg5ORtbKsUwlL2gQWEmhyFrI03qrY1layl_TfV94NyTG6jJj5nt7oEfKZwSUDVl39ArZiBVcMLlT9DYApKKoTsmC15EXJS3ZKFq_IGTlP6Q_ksxJsQfxDxM73fjDxH8W96SYz-jDQ0NLxN9Ip4XzFLo9GdHQXMaUpIh0DNdbmfsz9GY19KMKzd1m-R2q2fthSP1Ab-l1IfsT0kXxoTZfw00tdkqcfN4_r22Jz__Nufb0pLK_kWKA1rnWApuEgpawaaFBUjXC1KkvJmlpwdCvM5uWqrZUCEAJcUzPBrZSC8yX5enx3F8PfCdOoe5_ypp0ZMExJlxJqBaXKoDiCNoaUIrZ6F32fc9AM9BysPgSr59S0qvUhWF1l3ZcXA5Os6dpoBuvTmzgvWkmWse9HDPNn9x6jTtbjYNH5iHbULvh3jP4DxTqOgg</recordid><startdate>19990101</startdate><enddate>19990101</enddate><creator>Tsotsis, Thomas K.</creator><creator>Keller, Scott</creator><creator>Bardis, Jason</creator><creator>Bish, Jack</creator><general>Elsevier Ltd</general><general>Elsevier Science</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7SE</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>19990101</creationdate><title>Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites</title><author>Tsotsis, Thomas K. ; Keller, Scott ; Bardis, Jason ; Bish, Jack</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1999</creationdate><topic>Applied sciences</topic><topic>Exact sciences and technology</topic><topic>Forms of application and semi-finished materials</topic><topic>Laminates</topic><topic>Polymer industry, paints, wood</topic><topic>Technology of polymers</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Tsotsis, Thomas K.</creatorcontrib><creatorcontrib>Keller, Scott</creatorcontrib><creatorcontrib>Bardis, Jason</creatorcontrib><creatorcontrib>Bish, Jack</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Corrosion Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Polymer degradation and stability</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Tsotsis, Thomas K.</au><au>Keller, Scott</au><au>Bardis, Jason</au><au>Bish, Jack</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites</atitle><jtitle>Polymer degradation and stability</jtitle><date>1999-01-01</date><risdate>1999</risdate><volume>64</volume><issue>2</issue><spage>207</spage><epage>212</epage><pages>207-212</pages><issn>0141-3910</issn><eissn>1873-2321</eissn><coden>PDSTDW</coden><abstract>A study was conducted to evaluate the use of elevated pressure to accelerate the rate of thermo-oxidative degradation in polymeric composite materials. The motivation for this work was based on earlier studies by Tsotsis [1, 2], Kerr and Haskins [3]and by Ciutacu, et al. [4]which demonstrated that higher pressures of air or oxygen tended to increase the rate of degradation of polymeric composites. Moreover, accelerated aging methods are needed to evaluate materials which are to be used under long-term exposure to elevated temperature in oxidative environments such as the High-Speed Civil Transport (HSCT). The methodology proposed herein augments elevated temperature aging with elevated pressure to accelerate the rate of thermo-oxidative degradation. Temperatures below those used by previous workers were employed in order to avoid anomalous non-linear effects which can occur near the glass-transition temperature of polymeric materials. In the present work, Hexcel AS4/3501-6 [±45°] 2 s shear and [+45°/0°/−45°/90°] 2 s quasi-isotropic Hexcel IM7/8552 open hole compression specimens were aged at 121°C (250°F) at pressures of 0.101, 0.345, 1.03, and 1.72 MPa (14.7, 50, 150, and 250 psi). Three pressure vessels were designed and built to contain the prescribed pressures. These vessels were placed inside an oven and used an air bleed to recycle the air inside the vessels. For the open hole testing, a test method was derived from Boeing BSS 7260 to reduce the material required for each specimen. Specimens were tested as-made and after 1000 h exposure to each of the pressures. Results show up to a 20% reduction in tensile shear strength for the [±45°] 2 s specimens but show no decrease in open hole compression strength though weight losses and visible discoloration of the specimens are present in both materials. Differences are attributed to the different lay-ups used as well as the different materials systems of the two specimen types.</abstract><cop>Oxford</cop><pub>Elsevier Ltd</pub><doi>10.1016/S0141-3910(98)00190-6</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0141-3910
ispartof Polymer degradation and stability, 1999-01, Vol.64 (2), p.207-212
issn 0141-3910
1873-2321
language eng
recordid cdi_proquest_miscellaneous_27089029
source Elsevier
subjects Applied sciences
Exact sciences and technology
Forms of application and semi-finished materials
Laminates
Polymer industry, paints, wood
Technology of polymers
title Preliminary evaluation of the use of elevated pressure to accelerate thermo-oxidative aging in composites
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T06%3A41%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Preliminary%20evaluation%20of%20the%20use%20of%20elevated%20pressure%20to%20accelerate%20thermo-oxidative%20aging%20in%20composites&rft.jtitle=Polymer%20degradation%20and%20stability&rft.au=Tsotsis,%20Thomas%20K.&rft.date=1999-01-01&rft.volume=64&rft.issue=2&rft.spage=207&rft.epage=212&rft.pages=207-212&rft.issn=0141-3910&rft.eissn=1873-2321&rft.coden=PDSTDW&rft_id=info:doi/10.1016/S0141-3910(98)00190-6&rft_dat=%3Cproquest_cross%3E27089029%3C/proquest_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c367t-ecadfd0eab307776b0be56b5d892271b853ed4eacc24f89900550db8153c77533%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=27089029&rft_id=info:pmid/&rfr_iscdi=true