Congruent MgO:LiNbO3 single crystals doped with 0, 2.5, 5.0, 7.5 and 10.0 mol% of MgO were grown by the Czochralski method. The grown crystals were water clear without any precipitation. Their density and Curie temperature (Tc) were measured. The Curie temperature increased first with the MgO concen...

Full description

Saved in:
Bibliographic Details
Published in:Materials letters 1995-06, Vol.24 (1-3), p.157-160
Main Authors: KIM, I. W, PARK, B. C, JIN, B. M, BHALLA, A. S, KIM, J. W
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Congruent MgO:LiNbO3 single crystals doped with 0, 2.5, 5.0, 7.5 and 10.0 mol% of MgO were grown by the Czochralski method. The grown crystals were water clear without any precipitation. Their density and Curie temperature (Tc) were measured. The Curie temperature increased first with the MgO concentration and decreased again when the concentration of MgO went beyond the threshold limit ((Mg)c, 5.0-7.5 mol%). Optical absorption edge and IR absorption spectra were measured at room temperature. The threshold concentration of nearly 6.0 mol% was estimated. The IR absorption peak appeared at 3470 cm-1 in 0-5.0 mol% and at 3534 cm-1 in 7.5-10.0 mol%; the peak shifted about 60 cm-1 towards the shorter wavelength side. 15 refs.