Low temperature sintering of La(Ca)CrO3 prepared by an autoignition process

Ultrafine powders of calcium substituted lanthanum chromite with average particle size of 0.57 micron, synthesised by a simple process of autoignition of citrate-nitrate gels, can be sintered at relatively low temperatures (1200-1250 C) compared to those normally reported. The sintered samples show...

Full description

Saved in:
Bibliographic Details
Published in:Materials letters 2000-09, Vol.45 (3-4), p.162-166
Main Authors: CHAKRABORTY, A, BASU, R. N, MAITI, H. S
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Ultrafine powders of calcium substituted lanthanum chromite with average particle size of 0.57 micron, synthesised by a simple process of autoignition of citrate-nitrate gels, can be sintered at relatively low temperatures (1200-1250 C) compared to those normally reported. The sintered samples show adequate electrical conductivity and thermal expansion behaviour at 1000 C for use as an interconnect material for solid oxide fuel cells. 25 refs.
ISSN:0167-577X
1873-4979
DOI:10.1016/S0167-577X(00)00098-7