Loading…

Performance of monolithic and TiB2 reinforced MoSi2 in dry sliding contact with steel

MoSi2 and its composite with TiB2 (10 and 20 wt%) particulates were synthesised by hot pressing. Dry sliding wear experiments were done on these samples by the pin-on-disc method on an EN-24 steel disc. It was observed that the densification and the reinforcement of the matrix are beneficial in redu...

Full description

Saved in:
Bibliographic Details
Published in:Materials letters 2002-04, Vol.53 (4-5), p.379-383
Main Authors: Jayasingh, E.Moses, Tantri, P.Srikari, Bhaskaran, T.A, Biswas, S.K, Ramasesha, Sheela K
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:MoSi2 and its composite with TiB2 (10 and 20 wt%) particulates were synthesised by hot pressing. Dry sliding wear experiments were done on these samples by the pin-on-disc method on an EN-24 steel disc. It was observed that the densification and the reinforcement of the matrix are beneficial in reducing the friction and wear of MoSi2. The tribofilm that was formed during sliding contained both the disc and the pin material. 13 refs.
ISSN:0167-577X
DOI:10.1016/S0167-577X(01)00511-0