To analyze simplified adhesive containing pure or silanized bioglass 45S5 (with calcium) or Sr-45S5 (strontium-substituted) fillers applied on dentin and to evaluate the microtensile bond strength (µTBS), interface nanoleakage, degree of conversion of adhesive, collagen degradation and remineralizat...

Full description

Saved in:
Bibliographic Details
Published in:Dental materials 2023-02, Vol.39 (2), p.217-226
Main Authors: Rifane, Tainah Oliveira, Cordeiro, Karen Evellin Moura, Silvestre, Francisbênia Alves, Souza, Marina Trevelin, Zanotto, Edgar Dutra, Araújo-Neto, Vitaliano Gomes, Giannini, Marcelo, Sauro, Salvatore, de Paula, Diego Martins, Feitosa, Victor Pinheiro
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:To analyze simplified adhesive containing pure or silanized bioglass 45S5 (with calcium) or Sr-45S5 (strontium-substituted) fillers applied on dentin and to evaluate the microtensile bond strength (µTBS), interface nanoleakage, degree of conversion of adhesive, collagen degradation and remineralization. Ambar Universal adhesive (FGM) was doped with 10 wt% bioactive glasses to form following groups: Control (no bioglass), 45S5 (conventional bioglass 45S5), Sr-45S5 (Sr-substituted bioglass 45S5), Sil-45S5 (silanized bioglass 45S5) and Sil-Sr-45S5 (silanized bioglass Sr-45S5). Adhesives were applied after dentin acid-etching using phosphoric acid at extracted human molars. Resin-dentin sticks were obtained and tested for µTBS, nanoleakage at 24 h or 6 months. Degree of conversion was measured using micro-Raman spectroscopy. Dentin remineralization was assessed by FTIR after 6-month storage in PBS. Hydroxyproline (HYP) release was surveyed by UV-Vis spectroscopy. Statistical analysis was performed using ANOVA and Tukey’s test (p  0.05). Control (p = 0.018) and Sil-Sr-45S5 (p 