Development of a new alkali resistant coating
The effect of different new sol-gel BaO—TiO2—SiO2 and CaO—BaO—TiO2—SiO2 coatings on long-term durability of glass fiber reinforced cement (GRC) was examined. Flexural strength of GRC was measured after curing for 7 to 150 days. Significant improvement was observed for coated GRC in this study and di...
Saved in:
Published in: | Journal of sol-gel science and technology 2003-07, Vol.27 (3), p.309-313 |
---|---|
Main Authors: | , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The effect of different new sol-gel BaO—TiO2—SiO2 and CaO—BaO—TiO2—SiO2 coatings on long-term durability of glass fiber reinforced cement (GRC) was examined. Flexural strength of GRC was measured after curing for 7 to 150 days. Significant improvement was observed for coated GRC in this study and discussed in terms of the hydrate formation at interface. Concerned with the alkali resistance, CaO—BaO—TiO2—SiO2 coating was more effective than BaO—TiO2—SiO2 coating. In special, the 10CaO—10BaO—60TiO2—20SiO2 coating, prepared by sol-gel method, was recommended for the highest flexural strength of GRC and least corrosion at surface of E-glass fiber. |
---|---|