Infrared Detectors with Poly(3,4-ethylenedioxy thiophene)/Poly(styrene sulfonic acid) (PEDOT/PSS) as the Active Material

Fast‐response large‐area plastic infrared detectors (see Figure (Wheatstone bridge configuration)) made from a conducting PEDOT/PSS film achieve a detectivity close to 105 cm √Hz W–1 at 1.18 eV. The nanosecond response arises from the direct absorption of infrared light by the charge carriers on the...

Full description

Saved in:
Bibliographic Details
Published in:Advanced materials (Weinheim) 2003-04, Vol.15 (7-8), p.613-616
Main Authors: Meskers, S.C.J., van Duren, J.K.J., Janssen, R.A.J., Louwet, F., Groenendaal, L.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Fast‐response large‐area plastic infrared detectors (see Figure (Wheatstone bridge configuration)) made from a conducting PEDOT/PSS film achieve a detectivity close to 105 cm √Hz W–1 at 1.18 eV. The nanosecond response arises from the direct absorption of infrared light by the charge carriers on the polymer chain. The recovery of the device after illumination is much slower and is governed by heat transport from the polymer.
ISSN:0935-9648
1521-4095
DOI:10.1002/adma.200304592