Low Temperature Synthesis of Spinel Powders by Mechanical Grinding
Low temperature synthesis of spinel powder via intense mechanical grinding was performed. A dramatic decrease in the synthesis temperatures of ground powders was achieved. We were able to produce partially crystallized spinel at room temperature via a 110 minute grinding. Characterization of the syn...
Saved in:
Published in: | Key engineering materials 2004-01, Vol.264-268, p.53-56 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Low temperature synthesis of spinel powder via intense mechanical grinding was performed. A dramatic decrease in the synthesis temperatures of ground powders was achieved. We were able to produce partially crystallized spinel at room temperature via a 110 minute grinding. Characterization of the synthesized powders was performed using SEM, XRD and DTA. Each stage of synthesis was analyzed using these techniques. Mixtures of Mg(OH)2 and Al(OH)3 were used for synthesis. Temperatures as low as 800 deg C were able to produce bumps in the XRD patterns of ground powders at the 20 angles for spinel crystals. |
---|---|
ISSN: | 1013-9826 1662-9795 1662-9795 |
DOI: | 10.4028/www.scientific.net/KEM.264-268.53 |