Fabrication of Sm1Ba2Cu3O7 coated conductors using the co-evaporation method
We fabricated a coated conductor 7.5 m long and 9 mm wide using a biaxially textured Ni tape. The standard buffer layers, CeO2/Y SZ/CeO2, were used. A thick Sm1Ba2Cu3O7 (SBCO) film was deposited using the co-evaporation method, followed by in situ deposition of an Ag protection layer. The whole leng...
Saved in:
Published in: | Superconductor science & technology 2004-04, Vol.17 (4), p.580-584 |
---|---|
Main Authors: | , , , , , |
Format: | Article |
Language: | English |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | We fabricated a coated conductor 7.5 m long and 9 mm wide using a biaxially textured Ni tape. The standard buffer layers, CeO2/Y SZ/CeO2, were used. A thick Sm1Ba2Cu3O7 (SBCO) film was deposited using the co-evaporation method, followed by in situ deposition of an Ag protection layer. The whole length of SBCO film was deposited in a single batch process, which took 7 h. We checked the distribution of critical currents (Ic) by I-V measurements in all the sections comprising the tape. Ic at 77 K was 90-130 A in most parts of the whole length. |
---|---|
ISSN: | 0953-2048 1361-6668 |
DOI: | 10.1088/0953-2048/17/4/002 |