Manipulating Magnetoresistance Near Room Temperature in La0.67Sr0.33MnO3/La0.67Ca0.33MnO3 Films Prepared by Polymer Assisted Deposition

Multilayer‐coated La0.67Sr0.33MnO3/La0.67Ca0.33MnO3 (LSMO/LCMO) films can be prepared using cost‐effective polymer assisted deposition, keeping a constant LSMO/LCMO volume ratio. By changing the thickness of the individual layers (see figure), the temperature of maximum resistance and the magnitude...

Full description

Saved in:
Bibliographic Details
Published in:Advanced materials (Weinheim) 2006-10, Vol.18 (20), p.2695-2698
Main Authors: Jain, M., Shukla, P., Li, Y., Hundley, M. F., Wang, H., Foltyn, S. R., Burrell, A. K., McCleskey, T. M., Jia, Q. X.
Format: Article
Language:English
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Multilayer‐coated La0.67Sr0.33MnO3/La0.67Ca0.33MnO3 (LSMO/LCMO) films can be prepared using cost‐effective polymer assisted deposition, keeping a constant LSMO/LCMO volume ratio. By changing the thickness of the individual layers (see figure), the temperature of maximum resistance and the magnitude of magnetoresistance values can be manipulated. Similar properties are not achieved by simply mixing LSMO with LCMO phases at the same volume ratio.