Sintering Al2O3-Cr Composites Made From Micro- and Nanopowders
This paper presents the results of studies on sintering Al2O3-Cr composites of different chemical compositions (from 25 to 75 vol.% of each component). The factor analyzed was the influence of time (from 15 to 60 min.), temperature (from 1200-16000, pressure (0.5 and 30 MPa) and powder graining (for...
Saved in:
Published in: | Science of sintering 2004-09, Vol.36 (3), p.171-177 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | This paper presents the results of studies on sintering Al2O3-Cr composites of different chemical compositions (from 25 to 75 vol.% of each component). The factor analyzed was the influence of time (from 15 to 60 min.), temperature (from 1200-16000, pressure (0.5 and 30 MPa) and powder graining (for Al2O3 powders 80nm or 1um) on the density of sinters obtained. It was found that nanopowder composites are characterized by a higher density (by about 1-2%) than the micropowder composite, the remaining conditions of the process intact. Using the pressure of 30MPa allows obtaining of a definite sintering degree at a temperature of about 200DGC lower than at a pressure of 0.5 MPa. |
---|---|
ISSN: | 0350-820X |
DOI: | 10.2298/SOS0403171P |