Impression Creep in TBC and Advanced Ceramics Materials

The indentation creep of free-standing Y-ZrO2 layer and 20Sc-60Si-20Mg-80O-20N oxynitride glass has been investigated. Creep experiment has been performed with flat cylindrical indenter (hot pressed SiC) in the temperature range from 860 °C to 1300 °C at the loads from 20 to 100 MPa. The strain-time...

Full description

Saved in:
Bibliographic Details
Published in:Key engineering materials 2007-01, Vol.333, p.281-284
Main Authors: Jan, Vít, Hegedűsová, Lucia, Dorčáková, Františka, Dusza, Ján
Format: Article
Language:English
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The indentation creep of free-standing Y-ZrO2 layer and 20Sc-60Si-20Mg-80O-20N oxynitride glass has been investigated. Creep experiment has been performed with flat cylindrical indenter (hot pressed SiC) in the temperature range from 860 °C to 1300 °C at the loads from 20 to 100 MPa. The strain-time relationship was registered and the creep exponent and activation energy of creep have been calculated. The microstructure changes have been observed and documented. Viscosity as a function of temperature and the glass transition temperature (Tg) were determined in oxynitride glass and compared with values from compressive creep.