Effects of Al3Sc particle size and precipitate-free zones on fatigue behavior and dislocation structure of an aged Al-Mg-Sc alloy

Al-Mg-Sc alloy polycrystals have been cyclically deformed at room temperature under constant stress amplitudes. Cyclic softening after initial hardening is found in specimens with small particles of 4nm, but no cyclic softening takes place in specimens with large particles of 11nm. Transmission elec...

Full description

Saved in:
Bibliographic Details
Published in:International journal of fatigue 2008-04, Vol.30 (4), p.635-641
Main Authors: WATANABE, C, MONZEN, R, TAZAKI, K
Format: Article
Language:English
Subjects:
Citations: Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Al-Mg-Sc alloy polycrystals have been cyclically deformed at room temperature under constant stress amplitudes. Cyclic softening after initial hardening is found in specimens with small particles of 4nm, but no cyclic softening takes place in specimens with large particles of 11nm. Transmission electron microscopy observations reveal that dislocations are uniformly distributed under all applied stress amplitudes in the specimens containing large particles, whereas clearly developed slip bands are formed in the cyclically softened specimens bearing small particles. Two-step aging causes a decrease in the width of precipitate-free zones in the large-particle specimen, resulting in the improvement of fatigue life.
ISSN:0142-1123
1879-3452
DOI:10.1016/j.ijfatigue.2007.05.010