Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys

The corrosion of commercial die-cast Mg–Al alloys was elucidated by a study, of the corrosion in 3% NaCl, of (i) high-pressure die-cast (HPDC) model Mg–Al alloys, (ii) low-purity Mg, (iii) high-purity (HP) Mg and (iv) HP Mg heat treated at 550 °C. HPDC is the most important route for the production...

Full description

Saved in:
Bibliographic Details
Published in:Corrosion science 2009-03, Vol.51 (3), p.602-619
Main Authors: Liu, Ming, Uggowitzer, Peter J., Nagasekhar, A.V., Schmutz, Patrik, Easton, Mark, Song, Guang-Ling, Atrens, Andrej
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The corrosion of commercial die-cast Mg–Al alloys was elucidated by a study, of the corrosion in 3% NaCl, of (i) high-pressure die-cast (HPDC) model Mg–Al alloys, (ii) low-purity Mg, (iii) high-purity (HP) Mg and (iv) HP Mg heat treated at 550 °C. HPDC is the most important route for the production of Mg components. The corrosion of the model alloys was dominated by the Fe impurity element. The present research identified the appearance of the Fe-rich particles in the microstructure. In high magnification (∼1000× to 5000×) secondary electron images, they appear as small white features, typically less than 1 μm in diameter. In order to understand the impurity tolerance limits, (i) the appropriate corrosion literature was summarised and reviewed and (ii) Mg phase diagrams were calculated using the Pandat software package. Calculated phase diagrams can explain (i) the tolerance levels for Fe and Cu and (ii) the production of high-purity castings by means of control of melt conditions; this has high significance for the production of quality castings from recycled Mg. A full analysis requires that the Mg database be extended to include Ni, Co and some RE. The Fe tolerance limit is ∼5–10 ppm for cast HP Mg heat treated at 550 °C. Analysis of the Mg corrosion literature indicates that several studies have been dominated by the Fe impurity content and have not dealt with the stated aims; it means that the full chemical composition should be reported in all studies of the corrosion of Mg alloys.
ISSN:0010-938X
1879-0496
DOI:10.1016/j.corsci.2008.12.015