Eu-doped BaTiO₃powder and film from sol-gel process with polyvinylpyrrolidone additive
Transparent BaTiO(3):Eu(3+) films were prepared via a sol-gel method and dip-coating technique, using barium acetate, titanium butoxide, and polyvinylpyrrolidone (PVP) as modifier viscosity. BaTiO(3):Eu(3+) films ~500 nm thick, crystallized after thermal treatment at 700 masculineC. The powders reve...
Saved in:
Published in: | International journal of molecular sciences 2009-09, Vol.10 (9), p.4088-4101 |
---|---|
Main Authors: | , , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Transparent BaTiO(3):Eu(3+) films were prepared via a sol-gel method and dip-coating technique, using barium acetate, titanium butoxide, and polyvinylpyrrolidone (PVP) as modifier viscosity. BaTiO(3):Eu(3+) films ~500 nm thick, crystallized after thermal treatment at 700 masculineC. The powders revealed spherical and rod shape morphology. The optical quality of films showed a predominant band at 615 nm under 250 nm excitation. A preliminary luminescent test provided the properties of the Eu(3+) doped BaTiO(3). |
---|---|