Water Sorption, Solubility and Dimensional Changes of Denture Base Polymers Reinforced with Short Glass Fibers

The aim of this study was to determine water sorption, solubility and dimensional stability of injection and compression-molded polymethyl methacrylate based denture base polymer that was reinforced with various concentrations and lengths of E-glass fibers. For water sorption and solubility, 20 test...

Full description

Saved in:
Bibliographic Details
Published in:Journal of biomaterials applications 2003-04, Vol.17 (4), p.321-335
Main Authors: Polat, Tülin N., Karacaer, Özgül, Tezvergil, Arzu, Lassila, Lippo V. J., Vallittu, Pekka K.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The aim of this study was to determine water sorption, solubility and dimensional stability of injection and compression-molded polymethyl methacrylate based denture base polymer that was reinforced with various concentrations and lengths of E-glass fibers. For water sorption and solubility, 20 test groups with different fiber contents and lengths of fibers were prepared. Test specimens without fibers were used as a control. The water sorption and solubility was measured after 90 days water storage. For dimensional stability, rhombic test specimens were prepared and the dimensional changes were measured after processing, drying and storing in water for 4 days and 30 days and were compared with those on the brass model. The water sorption and solubility of injection-molded denture base polymer was lower compared to compression-molded specimens (p0.05).
ISSN:0885-3282
1530-8022
DOI:10.1177/0885328203017004006