Increased dielectric breakdown strengths of melt-extruded polypropylene films

Melt-extruded polypropylene resin containing 1% or 2% ceresine wax yielded thin films that had significantly increased dielectric breakdown strengths but with virtually identical bulk dielectric properties. Ceresine wax acts as a trapping centre for electrons and by minimizing ionization of host pol...

Full description

Saved in:
Bibliographic Details
Published in:Polymer (Guilford) 1993-01, Vol.34 (5), p.1093-1094
Main Authors: Wade, William L, Mammone, Robert J, Binder, Michael
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Melt-extruded polypropylene resin containing 1% or 2% ceresine wax yielded thin films that had significantly increased dielectric breakdown strengths but with virtually identical bulk dielectric properties. Ceresine wax acts as a trapping centre for electrons and by minimizing ionization of host polypropylene molecules, dielectric breakdown strength is increased.
ISSN:0032-3861
1873-2291
DOI:10.1016/0032-3861(93)90234-2