Characterization of AZ PN114 resist for soft-x-ray projection lithography

Using 14-nm wavelength illumination, we have imaged 0.1-µm-wide lines and spaces in single-layer thin films of the highy sensitive, negative, chemically amplified resist AZ PN114 by usingboth a Schwarzschild 20× camera and an Offner ring field 1× optical system. For soft-x-ray projection lithography...

Full description

Saved in:
Bibliographic Details
Published in:Applied optics (2004) 1993-12, Vol.32 (34), p.7044-7049
Main Authors: Early, K, Tennant, D M, Jeon, D Y, Mulgrew, P P, Macdowell, A A, Wood Ii, O R, Kubiak, G D, Tichenor, D A
Format: Article
Language:English
Citations: Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c381t-35e1051f9a9be9305cafe348e9d214b4d982c3d3c54b56b398731ca841200a1c3
cites
container_end_page 7049
container_issue 34
container_start_page 7044
container_title Applied optics (2004)
container_volume 32
creator Early, K
Tennant, D M
Jeon, D Y
Mulgrew, P P
Macdowell, A A
Wood Ii, O R
Kubiak, G D
Tichenor, D A
description Using 14-nm wavelength illumination, we have imaged 0.1-µm-wide lines and spaces in single-layer thin films of the highy sensitive, negative, chemically amplified resist AZ PN114 by usingboth a Schwarzschild 20× camera and an Offner ring field 1× optical system. For soft-x-ray projection lithography the approximate 0.2-µm absorption length in resists at 14-nm wavelength necessitates a multilayer resist system. To explore further the requirements of the imaging layer of such a system, we have transferred patterns, exposed by a high-resolution electron beam in a 60-nm-thick layer of AZ PN114, into the underlying layers of a trilevel structure. Significant pattern edge noise and resist granularity were found. It remains to be determined whether the observed noise is dominated by statistical fluctuations in dose or by resist chemistry. We also investigated pinhole densities in these films and found them to increase from 0.2 cm(-2) for 380-mm-thick films to 15 cm(-2) for 50-nm-thick films.
doi_str_mv 10.1364/ao.32.007044
format article
fullrecord <record><control><sourceid>proquest_pubme</sourceid><recordid>TN_cdi_proquest_miscellaneous_755161387</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>755161387</sourcerecordid><originalsourceid>FETCH-LOGICAL-c381t-35e1051f9a9be9305cafe348e9d214b4d982c3d3c54b56b398731ca841200a1c3</originalsourceid><addsrcrecordid>eNo1jzFPwzAUhD2AaClszMgbU4pfnp3YY1VBqVQBA0iIJXpxHJoqrYvtSpRfTwVFN9zy3emOsSsQY8BC3pIfYz4WohRSnrAhKGUyyPXbgJ3HuBIClTTlGRvkQqvioCGbT5cUyCYXum9Knd9w3_LJO39-BJA8uNjFxFsfePRtyr6yQHu-DX7l7C_cd2npPwJtl_sLdtpSH93l0Ufs9f7uZfqQLZ5m8-lkkVnUkDJUDoSC1pCpnUGhLLUOpXamyUHWsjE6t9igVbJWRY1GlwiWtIRcCAKLI3bz13uY8blzMVXrLlrX97RxfherUikoAA-xEbs-krt67ZpqG7o1hX31_x5_AAaoWK4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>755161387</pqid></control><display><type>article</type><title>Characterization of AZ PN114 resist for soft-x-ray projection lithography</title><source>Optica Publishing Group Journals (Optical Society)</source><creator>Early, K ; Tennant, D M ; Jeon, D Y ; Mulgrew, P P ; Macdowell, A A ; Wood Ii, O R ; Kubiak, G D ; Tichenor, D A</creator><creatorcontrib>Early, K ; Tennant, D M ; Jeon, D Y ; Mulgrew, P P ; Macdowell, A A ; Wood Ii, O R ; Kubiak, G D ; Tichenor, D A</creatorcontrib><description>Using 14-nm wavelength illumination, we have imaged 0.1-µm-wide lines and spaces in single-layer thin films of the highy sensitive, negative, chemically amplified resist AZ PN114 by usingboth a Schwarzschild 20× camera and an Offner ring field 1× optical system. For soft-x-ray projection lithography the approximate 0.2-µm absorption length in resists at 14-nm wavelength necessitates a multilayer resist system. To explore further the requirements of the imaging layer of such a system, we have transferred patterns, exposed by a high-resolution electron beam in a 60-nm-thick layer of AZ PN114, into the underlying layers of a trilevel structure. Significant pattern edge noise and resist granularity were found. It remains to be determined whether the observed noise is dominated by statistical fluctuations in dose or by resist chemistry. We also investigated pinhole densities in these films and found them to increase from 0.2 cm(-2) for 380-mm-thick films to 15 cm(-2) for 50-nm-thick films.</description><identifier>ISSN: 1559-128X</identifier><identifier>DOI: 10.1364/ao.32.007044</identifier><identifier>PMID: 20856565</identifier><language>eng</language><publisher>United States</publisher><ispartof>Applied optics (2004), 1993-12, Vol.32 (34), p.7044-7049</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c381t-35e1051f9a9be9305cafe348e9d214b4d982c3d3c54b56b398731ca841200a1c3</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/20856565$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink></links><search><creatorcontrib>Early, K</creatorcontrib><creatorcontrib>Tennant, D M</creatorcontrib><creatorcontrib>Jeon, D Y</creatorcontrib><creatorcontrib>Mulgrew, P P</creatorcontrib><creatorcontrib>Macdowell, A A</creatorcontrib><creatorcontrib>Wood Ii, O R</creatorcontrib><creatorcontrib>Kubiak, G D</creatorcontrib><creatorcontrib>Tichenor, D A</creatorcontrib><title>Characterization of AZ PN114 resist for soft-x-ray projection lithography</title><title>Applied optics (2004)</title><addtitle>Appl Opt</addtitle><description>Using 14-nm wavelength illumination, we have imaged 0.1-µm-wide lines and spaces in single-layer thin films of the highy sensitive, negative, chemically amplified resist AZ PN114 by usingboth a Schwarzschild 20× camera and an Offner ring field 1× optical system. For soft-x-ray projection lithography the approximate 0.2-µm absorption length in resists at 14-nm wavelength necessitates a multilayer resist system. To explore further the requirements of the imaging layer of such a system, we have transferred patterns, exposed by a high-resolution electron beam in a 60-nm-thick layer of AZ PN114, into the underlying layers of a trilevel structure. Significant pattern edge noise and resist granularity were found. It remains to be determined whether the observed noise is dominated by statistical fluctuations in dose or by resist chemistry. We also investigated pinhole densities in these films and found them to increase from 0.2 cm(-2) for 380-mm-thick films to 15 cm(-2) for 50-nm-thick films.</description><issn>1559-128X</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1993</creationdate><recordtype>article</recordtype><recordid>eNo1jzFPwzAUhD2AaClszMgbU4pfnp3YY1VBqVQBA0iIJXpxHJoqrYvtSpRfTwVFN9zy3emOsSsQY8BC3pIfYz4WohRSnrAhKGUyyPXbgJ3HuBIClTTlGRvkQqvioCGbT5cUyCYXum9Knd9w3_LJO39-BJA8uNjFxFsfePRtyr6yQHu-DX7l7C_cd2npPwJtl_sLdtpSH93l0Ufs9f7uZfqQLZ5m8-lkkVnUkDJUDoSC1pCpnUGhLLUOpXamyUHWsjE6t9igVbJWRY1GlwiWtIRcCAKLI3bz13uY8blzMVXrLlrX97RxfherUikoAA-xEbs-krt67ZpqG7o1hX31_x5_AAaoWK4</recordid><startdate>19931201</startdate><enddate>19931201</enddate><creator>Early, K</creator><creator>Tennant, D M</creator><creator>Jeon, D Y</creator><creator>Mulgrew, P P</creator><creator>Macdowell, A A</creator><creator>Wood Ii, O R</creator><creator>Kubiak, G D</creator><creator>Tichenor, D A</creator><scope>NPM</scope><scope>7X8</scope></search><sort><creationdate>19931201</creationdate><title>Characterization of AZ PN114 resist for soft-x-ray projection lithography</title><author>Early, K ; Tennant, D M ; Jeon, D Y ; Mulgrew, P P ; Macdowell, A A ; Wood Ii, O R ; Kubiak, G D ; Tichenor, D A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c381t-35e1051f9a9be9305cafe348e9d214b4d982c3d3c54b56b398731ca841200a1c3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1993</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Early, K</creatorcontrib><creatorcontrib>Tennant, D M</creatorcontrib><creatorcontrib>Jeon, D Y</creatorcontrib><creatorcontrib>Mulgrew, P P</creatorcontrib><creatorcontrib>Macdowell, A A</creatorcontrib><creatorcontrib>Wood Ii, O R</creatorcontrib><creatorcontrib>Kubiak, G D</creatorcontrib><creatorcontrib>Tichenor, D A</creatorcontrib><collection>PubMed</collection><collection>MEDLINE - Academic</collection><jtitle>Applied optics (2004)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Early, K</au><au>Tennant, D M</au><au>Jeon, D Y</au><au>Mulgrew, P P</au><au>Macdowell, A A</au><au>Wood Ii, O R</au><au>Kubiak, G D</au><au>Tichenor, D A</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Characterization of AZ PN114 resist for soft-x-ray projection lithography</atitle><jtitle>Applied optics (2004)</jtitle><addtitle>Appl Opt</addtitle><date>1993-12-01</date><risdate>1993</risdate><volume>32</volume><issue>34</issue><spage>7044</spage><epage>7049</epage><pages>7044-7049</pages><issn>1559-128X</issn><abstract>Using 14-nm wavelength illumination, we have imaged 0.1-µm-wide lines and spaces in single-layer thin films of the highy sensitive, negative, chemically amplified resist AZ PN114 by usingboth a Schwarzschild 20× camera and an Offner ring field 1× optical system. For soft-x-ray projection lithography the approximate 0.2-µm absorption length in resists at 14-nm wavelength necessitates a multilayer resist system. To explore further the requirements of the imaging layer of such a system, we have transferred patterns, exposed by a high-resolution electron beam in a 60-nm-thick layer of AZ PN114, into the underlying layers of a trilevel structure. Significant pattern edge noise and resist granularity were found. It remains to be determined whether the observed noise is dominated by statistical fluctuations in dose or by resist chemistry. We also investigated pinhole densities in these films and found them to increase from 0.2 cm(-2) for 380-mm-thick films to 15 cm(-2) for 50-nm-thick films.</abstract><cop>United States</cop><pmid>20856565</pmid><doi>10.1364/ao.32.007044</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1559-128X
ispartof Applied optics (2004), 1993-12, Vol.32 (34), p.7044-7049
issn 1559-128X
language eng
recordid cdi_proquest_miscellaneous_755161387
source Optica Publishing Group Journals (Optical Society)
title Characterization of AZ PN114 resist for soft-x-ray projection lithography
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T13%3A42%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_pubme&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Characterization%20of%20AZ%20PN114%20resist%20for%20soft-x-ray%20projection%20lithography&rft.jtitle=Applied%20optics%20(2004)&rft.au=Early,%20K&rft.date=1993-12-01&rft.volume=32&rft.issue=34&rft.spage=7044&rft.epage=7049&rft.pages=7044-7049&rft.issn=1559-128X&rft_id=info:doi/10.1364/ao.32.007044&rft_dat=%3Cproquest_pubme%3E755161387%3C/proquest_pubme%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c381t-35e1051f9a9be9305cafe348e9d214b4d982c3d3c54b56b398731ca841200a1c3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=755161387&rft_id=info:pmid/20856565&rfr_iscdi=true