Ultrasonic and hardness measurements for ultrahigh pressure prepared WB ceramics

The Vickers hardness of pressure synthesized WB compacts was measured using a diamond indentation method. Under the applied load of 4.9 N, our test gave a maximum Vickers hardness of 30.1 GPa for WB compacts. The hardness of WC-8 wt.% Co composites was also measured under the same load for compariso...

Full description

Saved in:
Bibliographic Details
Published in:International journal of refractory metals & hard materials 2011-03, Vol.29 (2), p.329-331
Main Authors: Chen, Ying, He, Duanwei, Qin, Jiaqian, Kou, Zili, Bi, Yan
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The Vickers hardness of pressure synthesized WB compacts was measured using a diamond indentation method. Under the applied load of 4.9 N, our test gave a maximum Vickers hardness of 30.1 GPa for WB compacts. The hardness of WC-8 wt.% Co composites was also measured under the same load for comparison, which was found to be much lower than that of WB. The Young's modulus, bulk modulus, and shear modulus of WB and WC-8 wt.% Co were further investigated by ultrasonic measurements. The results suggest that WB might be a promising hard alloy material for industrial applications.
ISSN:0263-4368
2213-3917
DOI:10.1016/j.ijrmhm.2010.12.006