Loading…

Soft holographic interference lithography microlens for enhanced organic light emitting diode light extraction

Very uniform 2 μm-pitch square microlens arrays (μLAs), embossed on the blank glass side of an indium-tin-oxide (ITO)-coated 1.1 mm-thick glass, are used to enhance light extraction from organic light-emitting diodes (OLEDs) by ~100%, significantly higher than enhancements reported previously. The a...

Full description

Saved in:
Bibliographic Details
Published in:Optics express 2011-07, Vol.19 Suppl 4 (S4), p.A786-A792
Main Authors: Park, Joong-Mok, Gan, Zhengqing, Leung, Wai Y, Liu, Rui, Ye, Zhuo, Constant, Kristen, Shinar, Joseph, Shinar, Ruth, Ho, Kai-Ming
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Very uniform 2 μm-pitch square microlens arrays (μLAs), embossed on the blank glass side of an indium-tin-oxide (ITO)-coated 1.1 mm-thick glass, are used to enhance light extraction from organic light-emitting diodes (OLEDs) by ~100%, significantly higher than enhancements reported previously. The array design and size relative to the OLED pixel size appear to be responsible for this enhancement. The arrays are fabricated by very economical soft lithography imprinting of a polydimethylsiloxane (PDMS) mold (itself obtained from a Ni master stamp that is generated from holographic interference lithography of a photoresist) on a UV-curable polyurethane drop placed on the glass. Green and blue OLEDs are then fabricated on the ITO to complete the device. When the μLA is ~15 × 15 mm(2), i.e., much larger than the ~3 × 3 mm(2) OLED pixel, the electroluminescence (EL) in the forward direction is enhanced by ~100%. Similarly, a 19 × 25 mm(2) μLA enhances the EL extracted from a 3 × 3 array of 2 × 2 mm(2) OLED pixels by 96%. Simulations that include the effects of absorption in the organic and ITO layers are in accordance with the experimental results and indicate that a thinner 0.7 mm thick glass would yield a ~140% enhancement.
ISSN:1094-4087
1094-4087
DOI:10.1364/OE.19.00A786