Loading…

Anodic Behavior of White Iron Phases in Oxalic Media

Potential-pH diagrams of the iron-oxalic acid and ferric carbide-oxalic acid systems taking into account the equilibrium iron or ferric carbide and ferrous (II) oxalate are plotted. Kinetic investigations of the anodic dissolution of white iron, containing ferritic (99.975% Fe) and cementite (Fe^sub...

Full description

Saved in:
Bibliographic Details
Published in:Protection of metals 2004-01, Vol.40 (1), p.56-61
Main Authors: Saltykov, S. N., Makarov, G. V., Toroptseva, E. L., Filatova, Ya. B.
Format: Article
Language:English
Subjects:
Citations: Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Potential-pH diagrams of the iron-oxalic acid and ferric carbide-oxalic acid systems taking into account the equilibrium iron or ferric carbide and ferrous (II) oxalate are plotted. Kinetic investigations of the anodic dissolution of white iron, containing ferritic (99.975% Fe) and cementite (Fe^sub 3^C) phases, oxalic acid environment evidence that the alloy is passivated due to the formation of a FeC^sub 2^O^sub 4^ polylayer.[PUBLICATION ABSTRACT]