Hysteresis loops of polarization and magnetization in (BiNd0.05)(Fe0.97Mn0.03)O3/Pt/CoFe2O4 layered epitaxial thin film grown by pulsed laser deposition

(BiNd0.05)(Fe0.97Mn0.03)O3 (BNFM)/Pt/CoFe2O4 (CFO) layered thin film was fabricated on (100) SrTiO3 substrate by pulsed laser deposition. BNFM, Pt, and CFO layers were epitaxially grown on the substrate. Almost no increase of leakage current due to the formation of heteroepitaxial structure was foun...

Full description

Saved in:
Bibliographic Details
Published in:Thin solid films 2011-09, Vol.519 (22), p.7727-7730
Main Authors: KAWAE, Takeshi, JIE HU, NAGANUMA, Hiroshi, NAKAJIMA, Takeshi, TERAUCHI, Yuki, OKAMURA, Soichiro, MORIMOTO, Akiharu
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:(BiNd0.05)(Fe0.97Mn0.03)O3 (BNFM)/Pt/CoFe2O4 (CFO) layered thin film was fabricated on (100) SrTiO3 substrate by pulsed laser deposition. BNFM, Pt, and CFO layers were epitaxially grown on the substrate. Almost no increase of leakage current due to the formation of heteroepitaxial structure was found, and well-saturated hysteresis loops in the polarization vs electric field and magnetization vs magnetic field curves coexist at room temperature. The remnant polarization and remnant magnetization values were 55 mu C/cm2, and 70-145mA/m, respectively.