Loading…

Effect of Active Bonding Application after Selective Dentin Etching on the Immediate and Long-Term Bond Strength of Two Universal Adhesives to Dentin

The objective was to evaluate the influence of active bonding applications (ABA) for different time intervals after selective dentin etching (SDE) for 3 s on the microtensile bond strength (μTBS) to dentin of two universal adhesive systems (UAs): one containing 2-hydroxyethyl methacrylate (HEMA) (Sc...

Full description

Saved in:
Bibliographic Details
Published in:Polymers 2022-03, Vol.14 (6), p.1129
Main Authors: Hardan, Louis, Orsini, Giovana, Bourgi, Rim, Cuevas-Suárez, Carlos Enrique, Nicastro, Marco, Lazarescu, Florin, Filtchev, Dimitar, Cornejo-Ríos, Elizabeth, Zamarripa-Calderón, Juan Eliezer, Sokolowski, Krzysztof, Lukomska-Szymanska, Monika
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The objective was to evaluate the influence of active bonding applications (ABA) for different time intervals after selective dentin etching (SDE) for 3 s on the microtensile bond strength (μTBS) to dentin of two universal adhesive systems (UAs): one containing 2-hydroxyethyl methacrylate (HEMA) (Scotchbond Universal, SBU), and one that was HEMA-free (Prime&Bond Universal, PBU). Dentin bovine specimens were divided into four groups: self-etch as control (SE), SDE + ABA for 15 s (SDE15), SDE + ABA for 20 s (SDE20), and SDE + ABA for 25 s (SDE25). The μTBS test was performed after a water storage of 24 h and 6 months. Scanning electron microscopy (SEM) was used in order to examine the resin−dentin interface. For the PBU, the µTBS was significantly influenced only by the aging factor (p < 0.026). A statistically significant decrease in the µTBS after 6 months of aging was observed only for the SDE15 group. For SBU, µTBS was significantly influenced by the protocol application and the aging time (p ≤ 0.041). The groups SDE15, SDE20, and SDE25 achieved statistically significant higher values (after 24 h and 6 months). No considerable variances were noticed in the homogeneity and continuity of the hybrid layer (HL) among the groups. In conclusion, SDE and ABA improved the µTBS only of a HEMA-containing universal adhesive.
ISSN:2073-4360
2073-4360
DOI:10.3390/polym14061129