Leaching of nickel from Pomala’s reduced limonitic laterite using sulphuric acid

In present work, the experiment to extract nickel from Pomala’s reduced Limonitic Laterite nickel using aqueous sulphuric acid solutions has been done in laboratory scale experiment. The objective of experiment to investigate effect of temperature, sulfuric acid concentration, leaching time and oxyg...

Full description

Saved in:
Bibliographic Details
Main Authors: Prasetyo, Agus Budi, Setiawan, Iwan, Oediyani, Soesaptri, Irawan, Januar, Subagja, Rudi, Nabilah, Anissa, Lalasari, Latifa Hanum
Format: Conference Proceeding
Language:English
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In present work, the experiment to extract nickel from Pomala’s reduced Limonitic Laterite nickel using aqueous sulphuric acid solutions has been done in laboratory scale experiment. The objective of experiment to investigate effect of temperature, sulfuric acid concentration, leaching time and oxygen addition on nickel extraction from Pomala’s reduced Limonitic laterite nickel. The variable for experiment covering temperature from 60oC to 90oC, sulfuric acid concentration from 0.2 M to 1.0 M, leaching time from 60 minutes to 240 minutes and oxygen addition. The effect of those variables was observed to the nickel extraction process from Pomala’s reduced limonitic laterite nickel. The result of experiment shows 97.45 % of nickel was extracted from Pomala’s reduced Limonitic Laterite nickel by 1.0 M aqueous sulphuric acid solutions at temperature of 70oC.