Thaumasite formed by sulfate attack on mortar with limestone filler

Early evidence of thaumasite formation in mortar with limestone filler exposed to sulfate containing tunnel water in Norway is reviewed. The problem is discussed in light of the new European cement standard allowing cements containing up to 35% limestone (e.g. CEM II/B-L) rendering them prone to det...

Full description

Saved in:
Bibliographic Details
Published in:Cement & concrete composites 2003-12, Vol.25 (8), p.955-959
Main Author: Justnes, Harald
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Early evidence of thaumasite formation in mortar with limestone filler exposed to sulfate containing tunnel water in Norway is reviewed. The problem is discussed in light of the new European cement standard allowing cements containing up to 35% limestone (e.g. CEM II/B-L) rendering them prone to detrimental sulfate attack. Experiments are performed where mortars with 20% limestone or quartz filler, respectively, are stored in 5% sodium sulfate solution saturated with gypsum at 5 °C. Length change, flexural strength and compressive strength are measured periodically for a year. The microstructure of the mortars is inspected by scanning electron microscopy and energy dispersive analyser of X-rays documenting the formation of sulfate containing species including ettringite and thaumasite.
ISSN:0958-9465
1873-393X
DOI:10.1016/S0958-9465(03)00120-3