Dynamic oxidation protective ultrahigh temperature ceramic TaB2-20%wtSiC composite coating for carbon material
TaB2–20%wtSiC composite coating containing high content of TaB2 was synthesized by liquid phase sintering method to enhance the anti-oxidation property of the carbon materials. The coated sample exhibits a trend of sustained weight gain whose final value is about 1.35%, while there is no weight loss...
Saved in:
Published in: | Composites. Part B, Engineering Engineering, 2019-03, Vol.161, p.220-227 |
---|---|
Main Authors: | , , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | TaB2–20%wtSiC composite coating containing high content of TaB2 was synthesized by liquid phase sintering method to enhance the anti-oxidation property of the carbon materials. The coated sample exhibits a trend of sustained weight gain whose final value is about 1.35%, while there is no weight loss zone in weight loss rate curves, but a rapid weight gain region around 800 °C. The generated compound glass layer presents a structure of Ta-oxides/TaBSiO/SiO2 triple glass layer. The rough surface of top Ta-oxides layer increases the oxidation defensive area of the glass layer, while the self-sealing TaBSiO/SiO2 compound glass ceramics layer can arrest the microcracks, blocking the fast diffusion channel of oxygen. |
---|---|