Thermal treatment effect on electrochemical properties of silicon alloy anodes with poly(ether imide) binder for lithium-ion batteries

The development of silicon-based anodes with high capacity and good cycling stability for next-generation Li+ batteries (LIBs) is a very challenging task due to the large volume expansion of the electrodes during repeated cycling, which leads to fading in capacity. In this study, the electrochemical...

Full description

Saved in:
Bibliographic Details
Published in:Polymer (Guilford) 2023-07, Vol.280, p.126042, Article 126042
Main Authors: Mukhan, Orynbassar, Yun, Ji-Su, Kim, Eun Kyung, Ji, Sang-Gu, Umirov, Nurzhan, Lee, Byoung-Min, Jeong, Chang-Uk, Kim, Sung-Soo, Choi, Jae-Hak
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The development of silicon-based anodes with high capacity and good cycling stability for next-generation Li+ batteries (LIBs) is a very challenging task due to the large volume expansion of the electrodes during repeated cycling, which leads to fading in capacity. In this study, the electrochemical performance of Si alloy-based anodes with poly (ether imide) (PEI) binder is evaluated after thermal treatment at various temperatures. The systematic study revealed that the thermal treatment of the anodes with PEI binder at above 500 °C results in the partial carbonization of the PEI and remarkably enhances the electrochemical performance, such as cycle life and high rate capabilities. The partially carbonized PEI acts as both a binder and conductive additive for the Si-alloy anodes. This superior electrochemical performance is attributed to the strong adhesion of the partially carbonized PEI binder resulting from enhanced secondary interactions, which maintained good electrical contacts between the active materials, electronic conductors, and current collector during cycling. The partial carbonization strategy can be readily scaled up due to the facile heat treatment process, offering a new approach for developing next-generation high-capacity batteries. [Display omitted] •Thermal decomposition and partial carbonization of PEI binder at high temperatures.•Thermal treatment of Si@PEI effects on the high ICE and capacity of Si-based electrodes.•Good adhesive stable electrode structure for stable capacity retention.