Recovery of Cobalt in Sulfuric Acid Leaching Solution Using Oxalic Acid

Oxalic acid was used for recovering cobalt from leaching solution of spent lithium ion battery by precipitation method. Crushed powders containing LiCoO 2 of spent lithium ion battery were obtained by crushing, magnetic separation and screening process. These powders were dissolved in 2 M H 2 SO 4 s...

Full description

Saved in:
Bibliographic Details
Published in:Geosystem engineering 2006, 9(3), , pp.81-85
Main Authors: Sohn, Jeong-Soo, Yang, Dong-Hyo, Shin, Shun-Myung, Kang, Jin-Gu
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Oxalic acid was used for recovering cobalt from leaching solution of spent lithium ion battery by precipitation method. Crushed powders containing LiCoO 2 of spent lithium ion battery were obtained by crushing, magnetic separation and screening process. These powders were dissolved in 2 M H 2 SO 4 solution with H 2 O 2 as a reducing agent. After dissolving Co and Li components, the solution of oxalic acid was added. Co(II) in leaching solution could be removed in the form of insoluble oxalates. The precipitate formed was crystalline, compact and easily filtered. With the increase in oxalic acid, the rate of cobalt precipitate increased to 90% at 1:4 mole ratio of Co(II) and oxalic acid concentration. When cobalt ion was precipitated into cobalt oxalate, nickel and copper ions were co-precipitated but there were no co-precipitates of Li, Al and Fe. The amounts of Ni and Cu in the solutions were below 1%. After heat treatment of precipitates at above 250°C, cobalt oxalate was changed into cobalt oxide.