Loading…

Interfacial conduction mechanism of cesium hydrogen phosphate and silicon pyrophosphate composite electrolytes for intermediate-temperature fuel cells

As an electrolyte for intermediate-temperature fuel cells (ITFCs), which are operative at 200°C to 300°C, a composite electrolyte CsH5(PO4)2/SiP2O7 has been investigated. The CsH5(PO4)2/SiP2O7 composite is reported to exhibit higher conductivity than pure CsH5(PO4)2, possibly by forming a highly-con...

Full description

Saved in:
Bibliographic Details
Published in:Solid state ionics 2016-02, Vol.285, p.160-164
Main Authors: Kikuchi, Ryuji, Ogawa, Akari, Matsuoka, Takuya, Takagaki, Atsushi, Sugawara, Takashi, Oyama, S.Ted
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:As an electrolyte for intermediate-temperature fuel cells (ITFCs), which are operative at 200°C to 300°C, a composite electrolyte CsH5(PO4)2/SiP2O7 has been investigated. The CsH5(PO4)2/SiP2O7 composite is reported to exhibit higher conductivity than pure CsH5(PO4)2, possibly by forming a highly-conductive new phase at the interface between CsH5(PO4)2 and SiP2O7. In this study, we have prepared several SiP2O7 matrices of different surface properties, and studied the effect of the surface properties on the total conductivity as well as on the formation mechanism of the interfacial conductive phase. An effective medium approximation method was applied to the measured conductivity to analyze the interfacial conductive phase. Several SiP2O7 matrices of different acid properties and crystalline properties were fabricated, and the conductivity of the CsH5(PO4)2/SiP2O7 composite electrolyte was measured by AC impedance method. The acidity and crystallinity of the SiP2O7 matrices were found to be important properties for the formation of the interfacial conductive phase. The highest conductivity of the interfacial conductive phase was estimated to be 500mScm−1, which is almost three times larger than that of the pure CsH5(PO4)2, 160mScm−1. •The interfacial conduction mechanism of CsH5(PO4)2/SiP2O7 composite electrolyte was investigated.•High crystallinity of SiP2O7 resulted in enhanced conductivity and stability of CsH5(PO4)2/SiP2O7 composite electrolyte.•Acidic property of SiP2O7 was crucial for the formation of the interfacial conductive phase.•The conductivity of the interfacial conductive phase was estimated to be 500mScm−1 by effective medium approximation.